Method for manufacturing plastic elastomer injection moulded chopping board and integrated chopping board
A manufacturing method and elastic body technology, which can be applied to home appliances, applications, kitchen utensils, etc., can solve the problems of low adhesion between the plastic layer and the bamboo layer, single shape of the cutting board, and easy peeling, etc., to solve the problem of repeated cleaning and easy Depletion, aesthetic and stylish effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0032] Such as Figure 1-Figure 3 As shown, 100 is the bamboo part of the chopping board, 120 is the cut part, 140 is the digging groove, 160 is the hole, 200 is the glue coating, and 300 is the TPE plastic elastomer part. Figure 1-Figure 3 The bamboo-plastic integrated cutting board of the shape shown:
[0033] (1) Forming of bamboo boards,
[0034] (2) Glue the edges and corners of the upper and lower sides of the formed bamboo board, the thickness of the glue coating is 20 μm, and the glue used in the gluing is made by adding GPPS plastic to a solvent, wherein: the solvent is made of It is formed by mixing methyl ethyl ketone: methyl butyrophenone: xylene = 4:3:3 by volume, and the content of GPPS plastic is 5wt%; it is dried immediately after gluing, and injection molding is performed on the gluing part after drying.
[0035] (3) Inject the gluing part, where thermoplastic elastomer TPE (red) is used in the injection molding, the injection temperature is 180-190°C, and ...
Embodiment 2
[0038] Such as Figure 4 As shown in (a), 100 is the bamboo part of the cutting board, 160 is the hole, and 300 is the TPE plastic elastomer part, which is prepared according to the following method: Figure 4 (a) Bamboo-plastic integrated cutting board with the shape shown:
[0039] (1) Forming of bamboo boards,
[0040] (2) Glue the edges and corners of the upper and lower sides of the formed bamboo board, the thickness of the glue coating is 30 μm, and the glue used in the gluing is made by adding GPPS plastic to a solvent, wherein: the solvent is made of It is formed by mixing butanone:methyl butyrophenone:xylene=5:2:4 by volume, and the content of GPPS plastic is 10wt%; it is dried immediately after gluing, and the gluing part is injected after drying.
[0041] (3) Inject the gluing part, where thermoplastic elastomer TPE (purple) is used in the injection molding, the injection temperature is 210-220°C, and the injection pressure is 900kg / m 2 , the injection molding ti...
Embodiment 3
[0044] Such as Figure 4 As shown in (b), 100 is the wooden part of the cutting board, 140 is the groove, 160 is the hole, and 300 is the TPR plastic elastomer part, which is prepared according to the following method: Figure 4 (b) Wood-plastic integrated cutting board of the shape shown:
[0045] (1) Forming treatment of wooden boards,
[0046] (2) Glue the edges and corners of the upper and lower sides of the formed wooden board, and the thickness of the glue coating is 30 μm. The glue used in the gluing is made by adding GPPS plastic to a solvent, wherein: the solvent is made by pressing The volume ratio is methyl ethyl ketone: methyl butyrophenone: xylene = 3:2:2, and the content of GPPS plastic is 7wt%; it is dried immediately after gluing, and the gluing part is injected after drying.
[0047] (3) Inject the gluing part, where thermoplastic elastomer TPR (green) is used in the injection molding, the injection temperature is 190-200°C, and the injection pressure is 100...