A technology for penetrating crystal waterproofing and production technology, applied in rosin coatings, coatings and other directions, can solve the problems of short service life, easy aging, and high cost, and achieve the effect of reducing service life, extending waterproof service life, and enhancing service life.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
specific Embodiment approach 1
[0017] Its specific implementation mode one is:
[0018] 1. Remove impurities from raw materials by filtering;
[0019] 2. Mix the water and silane in the raw materials according to their weight ratio of 2:1 and then stir, put the stirred solution into the reactor and heat to 70°C, and then heat for 60 minutes;
[0020] 3. Add sodium abietate into the reactor according to 2% of the weight of the silane, and heat and stir for 30 minutes at a temperature of 70°C;
[0021] 4. Add sodium hydroxide into the reactor according to 50% of the weight of the silane, and heat and stir for 30 minutes at a temperature of 70°C;
[0022] 5. Lower the temperature to 50°C and stir for 30 minutes, adjust the pH value to 10, and cool naturally to form the waterproofing agent.
specific Embodiment approach 2
[0023] Its specific implementation mode two is:
[0024] 1. Remove impurities from raw materials by filtering;
[0025] 2. Mix the water and silane in the raw materials according to their weight ratio of 2:1 and then stir, put the stirred solution into the reactor and heat to 80°C for 60 minutes;
[0026] 3. Add sodium abietate into the reactor according to 2% of the weight of silane, and heat and stir for 30 minutes at 80°C;
[0027] 4. Add sodium hydroxide into the reactor according to 50% of the weight of silane, and heat and stir at 80°C for 30 minutes;
[0028] 5. Lower the temperature to 50°C and stir for 30 minutes, adjust the pH value to 11, and cool naturally to form the waterproofing agent.
specific Embodiment approach 3
[0029] Its specific implementation mode three is:
[0030] 1. Remove impurities from raw materials by filtering;
[0031] 2. Mix the water and silane in the raw materials according to their weight ratio of 2:1 and then stir, put the stirred solution into the reactor and heat to 75°C for 50 minutes;
[0032] 3. Add sodium abietate into the reactor according to 2% of the weight of silane, and heat and stir for 30 minutes at 75°C;
[0033] 4. Add sodium hydroxide into the reactor according to 50% of the weight of the silane, and heat and stir for 30 minutes at a temperature of 75°C;
[0034] 5. Lower the temperature to 60°C and stir for 30 minutes, adjust the pH value to 11, and cool naturally to form the waterproofing agent.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com