Low-temperature quick drying paint
A fast-drying paint and low-temperature technology, applied in the direction of coating, etc., can solve the problems that the paint can not be dried quickly, easy to scratch, delay time, etc., and achieve the effect that it is not easy to scratch and harmless to the human body
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
specific Embodiment 1
[0008] A low-temperature quick-drying coating, the low-temperature quick-drying coating is composed of the following components in parts by weight: 30 parts of hydroxyacrylic acid polymer, 1 part of polysiloxane, 12 parts of polycarbodiimide, and 8 parts of melamine resin , 7 parts of styrene, 3 parts of butyl acetate, 4 parts of propylene, 6 parts of butanol.
specific Embodiment 2
[0009] A low-temperature quick-drying coating, the low-temperature quick-drying coating is composed of the following components in parts by weight: 40 parts of hydroxyacrylic acid polymer, 10 parts of polysiloxane, 18 parts of polycarbodiimide, and 15 parts of melamine resin , 15 parts of styrene, 15 parts of butyl acetate, 17 parts of propylene, and 10 parts of butanol.
specific Embodiment 3
[0010] A low-temperature quick-drying coating, the low-temperature quick-drying coating is composed of the following components in parts by weight: 35 parts of hydroxyacrylic acid polymer, 7 parts of polysiloxane, 17 parts of polycarbodiimide, and 12 parts of melamine resin , 8 parts of styrene, 11 parts of butyl acetate, 15 parts of propylene, and 8 parts of butanol.