[0019] 1. Prescription for tannic acid ointment:
[0020] raw material Prescription amount Tannic acid 50g glycerin 50g sodium bisulfite 1g Glyceryl monostearate 120g beeswax 50g paraffin 50g Yellow Vaseline 50g liquid paraffin 250g Span 80 20g Tween 80 10g Ethylparaben 2g water Add to 1000g
[0021] 2. Preparation of tannic acid ointment:
[0022] Dissolve tannic acid with a small amount of ethanol or water, and then mix it with glycerin to obtain tannic acid glycerol solution. Glyceryl monostearate, beeswax, paraffin, yellow petrolatum, liquid paraffin and Span 80 were heated to 70°C, and stirred evenly to obtain an oil phase. The glycerol tannin solution, Tween 80, ethylparaben and water were heated to 70°C and stirred evenly to obtain an aqueous phase. Add the water phase to the oil phase, stir evenly while adding, condense and separate to obtain tannic acid ointment.
[0023] 3...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com