Novel solid wood skirting line and production method thereof
A baseboard and solid wood technology, applied in the field of building materials, can solve problems such as deformation and short service life, and achieve the effect of improving the quality of life and good waterproof effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0034] Example 1. A new type of solid wood skirting line, constituted as figure 1 As shown, comprising solid wood substrate 1, the surface of solid wood substrate 1 is provided with UV curing paint layer 2, PORELLE microporous film layer 3, glass fiber cloth layer 4 and flocking layer 5 successively; Consists of UV putty layer 6, UV elastic primer layer 7 and UV elastic topcoat layer 8 from inside to outside.
[0035] The method for manufacturing the aforementioned novel solid wood skirting line comprises the following steps:
[0036] ①Sanding the solid wood substrate;
[0037] ②Roller coating with UV water-based adhesive, drying; the drying temperature is 90-110°C, and the drying time is 50-70s;
[0038] ③ Roller coating of UV putty, semi-cured; the coating amount of UV putty is 20g / m 2 , the UV energy when semi-cured is 100mj / cm 2 ;
[0039] ④ Roller coating of UV elastic primer, curing; the coating amount of UV elastic primer is 20g / m 2 , the UV energy during curing ...
Embodiment 2
[0049] Example 2. A new type of solid wood skirting line, constituted as figure 1 As shown, comprising a solid wood substrate 1, the surface of the solid wood substrate 1 is successively provided with a UV curable paint layer 2, a PORELLE microporous film layer 3, a glass fiber cloth layer 4 and a flocking layer 5; the UV curable paint layer 2 Consists of UV putty layer 6, UV elastic primer layer 7 and UV elastic topcoat layer 8 from inside to outside.
[0050] The method for manufacturing the aforementioned novel solid wood skirting line comprises the following steps:
[0051] ①Sanding the solid wood substrate;
[0052] ②Roller coating with UV water-based adhesive and drying; the drying temperature is 90°C, and the drying time is 50s;
[0053] ③ Roller coating of UV putty, semi-cured; the coating amount of UV putty is 15g / m 2 , the UV energy when semi-cured is 90mj / cm 2 ;
[0054] ④ Roller coating of UV elastic primer, curing; the coating amount of UV elastic primer is ...
Embodiment 3
[0064] Example 3. A new type of solid wood skirting line, constituted as figure 1 As shown, comprising solid wood substrate 1, the surface of solid wood substrate 1 is provided with UV curing paint layer 2, PORELLE microporous film layer 3, glass fiber cloth layer 4 and flocking layer 5 successively; Consists of UV putty layer 6, UV elastic primer layer 7 and UV elastic topcoat layer 8 from inside to outside.
[0065] The method for manufacturing the aforementioned novel solid wood skirting line comprises the following steps:
[0066] ①Sanding the solid wood substrate;
[0067] ②Roller coating with UV water-based adhesive and drying; the drying temperature is 110°C, and the drying time is 70s;
[0068] ③ Roller coating of UV putty, semi-cured; the coating amount of UV putty is 25g / m 2 , the UV energy when semi-cured is 110mj / cm 2 ;
[0069] ④ Roller coating of UV elastic primer, curing; the coating amount of UV elastic primer is 25g / m 2 , the UV energy during curing is ...