Process for the preparation of iminodiacetic acid
A technology of iminodiacetic acid and iminodiacetic acid disodium salt, which is applied in the field of preparation of iminodiacetic acid, can solve the problems of high acid and alkali consumption, low conversion rate, serious problems, etc., and achieves high efficiency, simple reaction process and easy operation convenient effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0048] The concentration of iminodiacetic acid disodium salt is 5%, the temperature is 50°C, and the current density of S1 and S2 is 100 A / m 2 , The electrode spacing is 1.5cm, the cathode chamber and the intermediate chamber adopt sodium ion exchange membrane, the anolyte is 5% sulfuric acid, the anode DSA oxygen evolution electrode, the catholyte is 5% sodium hydroxide, and the cathode is a nickel-based active cathode. The flow rate was 0 mm / s, the solution was cycled and electrolyzed to pH 2, and the current efficiency was 97%.
Embodiment 2
[0050] The concentration of iminodiacetic acid disodium salt is 50%, the temperature is 90°C, and the current density of S1 and S2 is 1000 A / m 2 , The electrode spacing is 1.5 cm, the cathode chamber and the intermediate chamber adopt sodium ion exchange membrane, the anolyte is 5% sulfuric acid, the anode DSA oxygen evolution electrode, the catholyte is 5% sodium hydroxide, and the cathode is a nickel-based active cathode. The flow rate was 200 mm / s, the solution was electrolyzed in circulation until the pH was 0.1, and the current efficiency was 96%.
Embodiment 3
[0052] Iminodiacetic acid disodium salt concentration 40%, temperature 80°C, S1 current density 3000 A / m 2 , S2 current density is 1000 A / m 2 , The electrode spacing is 1.5 cm, the cathode chamber and the intermediate chamber adopt sodium ion exchange membrane, the anolyte is 5% sulfuric acid, the anode DSA oxygen evolution electrode, the catholyte is 5% sodium hydroxide, and the cathode is a nickel-based active cathode. The flow rate was 2 mm / s, the solution was electrolyzed to pH 1, and the current efficiency was 93%.