The technology of a steering wheel cover and a manufacturing method is applied to the steering control, handwheel, household components and other directions installed on the car, which can solve the problems of high temperature resistance, environmental protection, and non-recyclable use, so as to increase the availability. , The production method is simple, and the effect of relieving fatigue
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0031] The manufacturing method of steering wheel cover comprises the following steps:
[0032] (1) After heating the resin to 35°C, add a curing agent, mix well, spray it into the model of the massage part, obtain the massage part after casting, and perform demoulding treatment on the massage part;
[0033] (2) Heat the high molecular polymer to a temperature of 200°C, spray it into the anti-slip layer mold after melting, and fill the anti-slip layer mold;
[0034] (3) Pressure-hold the anti-slip layer mold as a whole in step (2) for 30 minutes to increase the density of the polymer in the anti-slip layer mould;
[0035] (4) The anti-slip layer mold in step (3) is cooled for the first time, and the temperature for the first time is 80°C;
[0036] (5) Demoulding the anti-slip layer mold that has undergone the first cooling treatment in step (4), to obtain an anti-slip layer with anti-slip lines on the inner surface;
[0037] (6) Take the elastic mesh and the massage part in ...
Embodiment 2
[0043]The manufacture method of steering wheel cover is the same as embodiment 1, and difference is:
[0044] In step (1), apply a release agent to the mold of the massage part before casting, and control the heating temperature at 25°C.
[0045] The heating temperature in step (2) is 160°C.
[0046] The pressure holding time in step (3) is 10 minutes.
[0047] The first cooling temperature in step (4) is 60°C.
[0048] The second cooling temperature in step (7) is 50°C.
Embodiment 3
[0050] The manufacture method of steering wheel cover is the same as embodiment 1, and difference is:
[0051] In step (1), apply a release agent to the mold of the massage part before casting, and control the heating temperature at 45°C.
[0052] The heating temperature in step (2) is 220°C.
[0053] The pressure holding time in step (3) is 40min.
[0054] In step (4), the first cooling temperature is 90°C.
[0055] The second cooling temperature in step (7) is 80°C.