A two-layer cowhide and craftsmanship technology, applied in dyeing, textiles and papermaking, etc., can solve the problems of complicated operation, great influence on the quality of finished leather, and high cost, and achieve the effect of simple operation control, less material consumption, and good quality
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0029] Step 1. Weigh the double-layer leather blank as the basis for the amount of water and other raw materials added in the subsequent process (the following are all based on the weight percentage of the double-layer leather blank). Throw the two-layer leather blank into the drum, and then go to step 2.
[0030] Step 2, return water
[0031] Add 45°C hot water of 300% of the weight of the two-layer leather blank to the drum, adjust the drum speed to 8rad / min, rotate for 90min, and drain.
[0032] Step 3, decolorization
[0033] Add 200% of the weight of the split leather at 50°C to the drum, then add 3% of the weight of the split leather to the weight of sodium carbonate, 6% of the weight of the split leather, sodium dithionite, turn Adjust the drum speed to 10rad / min, decolorize for 60min, wash with water until the floating color is removed, and drain.
[0034] Step 4. Retanning
[0035] Add 150% of the split leather weight of hot water at 30°C to the drum, then add 3% ...
Embodiment 2
[0045] Step 1. Weigh the double-layer leather blank as the basis for the amount of water and other raw materials added in the subsequent process (the following are all based on the weight percentage of the double-layer leather blank). Throw the two-layer leather blank into the drum, and then go to step 2.
[0046] Step 2, return water
[0047] Add 55°C hot water with 250% of the weight of the two-layer leather blank to the drum, adjust the drum speed to 8rad / min, rotate for 90min, and drain.
[0048] Step 3, decolorization
[0049] Add 150% of the split leather weight of hot water at 60°C to the drum, then add 2% of the split leather weight of sodium carbonate, 4% of the split leather weight of sodium dithionite, and adjust the drum speed to 10rad / min, decolorize for 60 min, wash with water until the floating color is removed, and drain.
[0050] Step 4. Retanning
[0051] Add 100% of the weight of the split leather blank at 40°C to the drum, then add 2% of the weight of ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com