A method for the preparation of pipe piles
A pipe pile and pile body technology, which is applied in the field of pipe pile preparation, can solve the problems of boiler explosion, high maintenance cost, and cost increase
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0065] A kind of embodiment of the preparation method of pipe pile described in the present invention, described method comprises the following steps:
[0066] Mix and stir the concrete raw materials to form the pile body concrete, put the mixed pile body concrete into the mold, carry out prestress tension, and centrifuge the pile body concrete after prestress tension until the pipe pile is formed, and the centrifugally formed pile concrete The prestressed concrete pipe pile is cured by atmospheric pressure steam, and then the mold is removed and naturally cured to obtain the pipe pile;
[0067] The normal-pressure steam curing includes the processes of static stop, temperature rise, constant temperature and temperature drop.
[0068] The resting time is 1 hour, the total time for heating up, constant temperature and temperature drop is 6 hours, and the constant temperature is 60°C.
[0069] The concrete comprises the following components by weight: 440 parts of cement, 660 p...
Embodiment 2
[0078] A kind of embodiment of the preparation method of pipe pile described in the present invention, described method comprises the following steps:
[0079] Mix and stir the concrete raw materials to form the pile body concrete, put the mixed pile body concrete into the mold, carry out prestress tension, and centrifuge the pile body concrete after prestress tension until the pipe pile is formed, and the centrifugally formed pile concrete The prestressed concrete pipe pile is cured by atmospheric pressure steam, and then the mold is removed and naturally cured to obtain the pipe pile;
[0080] The normal-pressure steam curing includes the processes of static stop, temperature rise, constant temperature and temperature drop.
[0081] The resting time is 1 hour, the total time for heating up, constant temperature and temperature drop is 6 hours, and the constant temperature is 65°C.
[0082] The concrete comprises the following components by weight: 480 parts of cement, 700 p...
Embodiment 3
[0091] A kind of embodiment of the preparation method of pipe pile described in the present invention, described method comprises the following steps:
[0092] Mix and stir the concrete raw materials to form the pile body concrete, put the mixed pile body concrete into the mold, carry out prestress tension, and centrifuge the pile body concrete after prestress tension until the pipe pile is formed, and the centrifugally formed pile concrete The prestressed concrete pipe pile is cured by atmospheric pressure steam, and then the mold is removed and naturally cured to obtain the pipe pile;
[0093] The normal-pressure steam curing includes the processes of static stop, temperature rise, constant temperature and temperature drop.
[0094] The resting time is 1 hour, the total time for heating up, constant temperature and temperature drop is 6 hours, and the constant temperature is 63°C.
[0095] The concrete comprises the following components by weight: 460 parts of cement, 680 p...
PUM
Property | Measurement | Unit |
---|---|---|
strength | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com