A modification method of ferrierite, a ferrierite and its application
A ferrierite and modification technology, applied to ferrierite and its application fields, can solve the problems of inability to obtain a catalyst, low conversion rate and selectivity, reduced selectivity, etc., and achieve low cost, simple method, and improved conversion rate. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0057] In this embodiment, the modification method provided by the present invention is used to treat ferrierite to obtain modified ferrierite.
[0058] Modification treatment: Take 90g of sodium ferrierite ZSM-23 (purchased from Shanghai Shentan Environmental Protection New Material Co., Ltd., the same below), and add it to 1000mL of a solution containing 32g of ammonium nitrate and 35.4g of ammonium fluorosilicate. Contact treatment at ℃ for 8h, then cooling, filtering, drying at 100℃ for 10h, and calcining at 500℃ for 4h to obtain modified ferrierite 1-A.
Embodiment 2
[0060] In this embodiment, the modification method provided by the present invention is used to treat ferrierite to obtain modified ferrierite.
[0061] Modification treatment: Take 90g of sodium ferrierite ZSM-35 (purchased from Dalian Ketelli Chemical Co., Ltd., the same below), add it to 1000mL solution containing 55.4g ammonium nitrate and 72g ammonium fluorosilicate, at 95°C After contacting for 7 hours, cooling, filtering, drying at 120°C for 8 hours, and calcining at 400°C for 6 hours, the modified ferrierite 2-A was obtained.
Embodiment 3
[0063] In this embodiment, the modification method provided by the present invention is used to treat ferrierite to obtain modified ferrierite.
[0064] Modification treatment: Take 90g of sodium ferrierite ZSM-38 (purchased from Shanghai Shentan Environmental Protection New Material Co., Ltd., the same below), and add it to 1000mL of a solution containing 9.4g of ammonium nitrate and 7.6g of ammonium fluorosilicate. Contact treatment at 75°C for 10 hours, cooling, filtration, drying at 90°C for 12 hours, and calcination at 600°C for 3 hours to obtain modified ferrierite 3-A.
PUM

Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com