preparation example Construction
[0033] see Figure 4 , the present invention further provides a method for preparing cigarette tipping paper, comprising:
[0034] S11, providing a base paper for tipping paper, the base paper for tipping paper has opposite first and second sides;
[0035] S12, providing an oil-repellent coating, printing or coating the oil-repellent coating on the first surface to obtain a first oil-repellent layer;
[0036] S13, providing an oleophobic and hydrophilic coating, the oleophobic and hydrophilic coating and the above-mentioned oil-repellent coating respectively have a compatible resin matrix;
[0037] S14, printing or coating the oleophobic and hydrophilic coating on the first oil-repellent layer to prepare a first oleophobic and hydrophilic layer, and obtaining the tipping paper for cigarettes.
[0038]In step S12, after the oil-repellent paint is printed or coated on the base paper of the tipping paper, all the solvents in the oil-repellent paint are volatilized, so as to obt...
Embodiment 1
[0058] The formula (mass percentage) of oleophobic hydrophilic coating in the present embodiment is as follows: 30% aqueous polycarbonate, 15% activated calcium carbonate, 25% ethanol, 26% water, 1% smooth agent, 1% anti-settling agent, 1% leveling agent, 1% defoamer.
[0059] The preparation method of described oleophobic hydrophilic coating is as follows:
[0060] (1) Mix ethanol and water and stir evenly to obtain a solution;
[0061] (2) adding water-based polycarbonate to the above solution, stirring evenly to obtain an emulsion;
[0062] (3) active calcium carbonate is added in the above-mentioned emulsion, stir evenly, obtain a suspension;
[0063] (4) Add slip agent, anti-sedimentation agent, defoamer, and leveling agent to the above-mentioned suspension;
[0064] (5) Sand mill the suspension obtained in step (4) for 60 min to obtain an oleophobic and hydrophilic coating with a fineness of 25 μm and a viscosity of 22 s (24° C., British 3# Charn cup).
[0065] The p...
Embodiment 2
[0070] The formula (mass percentage) of oleophobic hydrophilic coating in the present embodiment is as follows: 30% aqueous polycarbonate / polyurethane mixed emulsion, 15% talcum powder, 28% ethanol, 25% water, 0.5% smooth agent, 0.5% anti-corrosion Settling agent, 0.5% leveling agent, 0.5% defoamer.
[0071] The preparation method of described oleophobic hydrophilic coating is as follows:
[0072] (1) Mix ethanol and water and stir evenly to obtain a solution;
[0073] (2) adding the aqueous polycarbonate / polyurethane mixed emulsion to the above solution, stirring evenly to obtain an emulsion;
[0074] (3) Add talcum powder to the above-mentioned emulsion, stir evenly to obtain a suspension;
[0075] (4) Add slip agent, anti-sedimentation agent, defoamer, and leveling agent to the above-mentioned suspension;
[0076] (5) Sand mill the suspension obtained in step (4) for 60 minutes to obtain an oleophobic and hydrophilic coating with a fineness of 23 μm and a viscosity of 22...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More 