A kind of compound dephosphorization agent and preparation method thereof
A compound dephosphorization agent and dephosphorization agent technology, applied in chemical instruments and methods, water/sludge/sewage treatment, water/sewage treatment, etc., can solve problems such as the influence of the use system, and achieve expanded use range and simple use , a wide range of effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0036] A preparation method of a composite phosphorus removal agent, is characterized in that, comprises the steps:
[0037] Step 1. Add 400-600 parts by mass of water into the enamel reaction kettle, start stirring, slowly add industrial grade sulfuric acid into the reaction kettle, and adjust the pH to 1.0±0.1.
[0038] Step 2. Add 300-400 parts by mass of iron sulfate to the solution in step 1 to completely dissolve it.
[0039] Step 3, adding 80-120 parts by mass of aluminum sulfate to the solution in step 2 to completely dissolve it.
[0040] Step 4, adding 40-60 parts by mass of aluminum chloride to the solution in step 3 to completely dissolve it.
[0041] Step 5. Check the pH of the solution in step 4 to maintain the pH of the solution at 0.5-1.0. If the pH value is greater than 1.0, adjust it to 0.5-1.0 with industrial grade sulfuric acid.
[0042] Step 6. Completely filter the solution in step 5 with a 1200-1800 mesh acid-resistant filter.
[0043] Step 7, the sol...
Embodiment 1
[0046] A preparation method of a composite phosphorus removal agent, is characterized in that, comprises the steps:
[0047] Step 1. Add 500 parts by mass of water into the enamel reaction kettle, start stirring, slowly add industrial grade sulfuric acid into the reaction kettle, and adjust the pH to 1.0.
[0048] Step 2. Add 350 parts by mass of ferric sulfate to the solution in step 1 to completely dissolve it.
[0049] Step 3, adding 100 parts by mass of aluminum sulfate to the solution in step 2 to completely dissolve it.
[0050] Step 4. Add 50 parts by mass of aluminum chloride to the solution in step 3 to completely dissolve it.
[0051] Step 5. Check the pH of the solution in step 4 to maintain the pH of the solution at 0.8.
[0052] Step 6. Completely filter the solution in step 5 with a 1500-mesh acid-resistant filter.
[0053] Step 7, under the condition of 15r / min stirring of the solution filtered in step 6, add one-thousandth of polydimethyldiallylammonium chlori...
Embodiment 2
[0056] A preparation method of a composite phosphorus removal agent, is characterized in that, comprises the steps:
[0057] Step 1. Add 400 parts by mass of water into the enamel reaction kettle, start stirring, slowly add industrial grade sulfuric acid into the reaction kettle, and adjust the pH to 1.1.
[0058] Step 2. Add 300 parts by mass of ferric sulfate to the solution in step 1 to completely dissolve it.
[0059] Step 3, adding 80 parts by mass of aluminum sulfate to the solution in step 2 to completely dissolve it.
[0060] Step 4, adding 40 parts by mass of aluminum chloride to the solution in step 3 to completely dissolve it.
[0061] Step 5. Check the pH of the solution in step 4 to maintain the pH of the solution at 0.5.
[0062] Step 6. Completely filter the solution in step 5 with a 1200-mesh acid-resistant filter.
[0063] Step 7, under the condition of 15r / min stirring of the solution filtered in step 6, add one-thousandth of polydimethyldiallylammonium ch...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com