Inorganic coating and preparation method thereof
A technology of inorganic coatings and inorganic toners, applied in the chemical industry, can solve the problems of ineffective utilization of tailings materials and easy pollution of the environment, and achieve the effects of long service life, good non-fading, and good weather resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0022] The invention provides an inorganic coating, which is characterized in that it consists of the following components in mass percentage:
[0023]
[0024] Further, the additive is any one or a combination of two or more of plastic powder, cellulose, alkaline neutralizer, and anti-penetration agent.
[0025] The present invention also provides a method for preparing the above-mentioned inorganic coating, comprising the steps of:
[0026] 1) take each reaction substance according to weight percentage;
[0027] 2) Put the white cement, black cement, and tailings particles into a reaction container for stirring and mixing, then add the inorganic toner and the above-mentioned additives after 2-4 minutes, stir again, and pack after mixing evenly.
[0028] When the present invention is used, add clear water to the paint, the mass ratio of the clear water to the paint is 10-20:100, then fully stir; add oxalic acid solution to adjust the pH value to be neutral, and then use a...
Embodiment 2
[0030] The invention provides an inorganic coating, which is characterized in that it consists of the following components in mass percentage:
[0031]
[0032] Further, the additive is any one or a combination of two or more of plastic powder, cellulose, alkaline neutralizer, and anti-penetration agent.
[0033] The present invention also provides the preparation method of above-mentioned a kind of inorganic coating, comprises the following steps:
[0034] 1) take each reaction substance according to weight percentage;
[0035] 2) Put the white cement, black cement, and tailings particles into a reaction container for stirring and mixing, then add the inorganic toner and the above-mentioned additives after 2-4 minutes, stir again, and pack after mixing evenly.
[0036] When the present invention is used, add clear water to the paint, the mass ratio of the clear water to the paint is 10-20:100, then fully stir; add oxalic acid solution to adjust the pH value to be neutral,...
Embodiment 3
[0038] The invention provides an inorganic coating, which is characterized in that it consists of the following components in mass percentage:
[0039]
[0040] Further, the additive is any one or a combination of two or more of plastic powder, cellulose, alkaline neutralizer, and anti-penetration agent.
[0041] The present invention also provides the preparation method of above-mentioned a kind of inorganic coating, comprises the following steps:
[0042] 1) take each reaction substance according to weight percentage;
[0043] 2) Put the white cement, black cement, and tailings particles into a reaction container for stirring and mixing, then add the inorganic toner and the above-mentioned additives after 2-4 minutes, stir again, and pack after mixing evenly.
[0044] When the present invention is used, add clear water to the paint, the mass ratio of the clear water to the paint is 10-20:100, then fully stir; add oxalic acid solution to adjust the pH value to be neutral,...