Anti-condensation coating for sinks
An anti-condensation and coating technology, applied in the coating and other directions, can solve the problems of rough appearance of the paint film, rough production and processing, and peeling of the paint film, and achieve the effect of smooth appearance and high adhesion of the paint film.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] The water tank anti-condensation coating of the present invention comprises the following various components in parts by mass: 300 parts of water, 15 parts of dispersant, 1 part of wetting agent, 15 parts of antifreeze, 3 parts of defoamer, and film-forming aid 10 parts, 5 parts of titanium dioxide, 300 parts of shell powder, 200 parts of diatomaceous earth, 2 parts of pH regulator, 100 parts of hollow glass microspheres, 300 parts of emulsion, 3 parts of fungicide.
Embodiment 2
[0017] The anti-condensation coating for the sink comprises the following components in parts by mass: 400 parts of water, 10 parts of dispersant, 2 parts of wetting agent, 10 parts of antifreeze, 5 parts of defoamer, and 5 parts of film-forming aid , 10 parts of titanium dioxide, 200 parts of shell powder, 300 parts of diatomaceous earth, 1 part of pH regulator, 200 parts of hollow glass microspheres, 200 parts of emulsion, and 5 parts of fungicide.
Embodiment 3
[0019] The anti-condensation coating for the sink comprises the following components in parts by mass: 350 parts of water, 12.5 parts of dispersant, 1.5 parts of wetting agent, 12.5 parts of antifreeze, 4 parts of defoamer, and 7.5 parts of film-forming aid , 7.5 parts of titanium dioxide, 250 parts of shell powder, 250 parts of diatomaceous earth, 1.5 parts of pH regulator, 150 parts of hollow glass microspheres, 250 parts of emulsion, and 4 parts of bactericide.
[0020] Among the above-mentioned embodiments 1-3, the production process of the anti-condensation coating for the sink comprises the following steps:
[0021] Step 1. Add various components in sequence according to the above components, start the disperser and control the speed at 500r / min, then add dispersant, wetting agent, antifreeze, defoamer, film-forming aid, and stir for 15 minutes;
[0022] Step 2. After step 1 is completed, add titanium dioxide, shell powder, and diatomaceous earth in sequence, and dispers...
PUM
Login to View More Abstract