Preparation method of high-strength concrete separation wall
A concrete and separation wall technology, applied in the field of concrete building materials, can solve the problems of poor thermal insulation performance of solid clay bricks, large amount of bricks used in brick-concrete structures, and adverse environmental effects, and achieve low cost, strong bearing capacity, and scientific methods Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] A kind of preparation method of high-strength concrete partition wall described in the present embodiment, comprises the following steps:
[0016] (1) Material preparation: The raw materials include by weight: 160 parts of cement, 55 parts of slag, 11 parts of PPR powder, 5 parts of grinding wheel ash, 8 parts of sand, 1 part of thickener, and 280 parts of water;
[0017] (2) Heat the slag, PPR powder and grinding wheel ash to 145°C and stir for 20 minutes;
[0018] (3) Put the mixture of step (2), the thickener, and half of the water into the mixing tank and mix for 15 minutes;
[0019] (4) Put the cement, sand and remaining water into the mixing tank and mix for 18 minutes;
[0020] (5) Transport the uniformly mixed concrete to the site or precast workshop for pouring.
Embodiment 2
[0022] A kind of preparation method of high-strength concrete partition wall described in the present embodiment, comprises the following steps:
[0023] (1) Material preparation: The raw materials include by weight: 120 parts of cement, 70 parts of slag, 6 parts of PPR powder, 7 parts of grinding wheel ash, 5 parts of sand, 2 parts of thickener, and 250 parts of water;
[0024] (2) Heat slag, PPR powder and grinding wheel ash to 150°C and stir for 15 minutes;
[0025] (3) Put the mixture of step (2), thickener, and half of the water into the mixing tank and mix for 20 minutes;
[0026] (4) Put the cement, sand and remaining water into the mixing tank and mix for 15 minutes;
[0027] (5) Transport the uniformly mixed concrete to the site or precast workshop for pouring.
Embodiment 3
[0029] A kind of preparation method of high-strength concrete partition wall described in the present embodiment, comprises the following steps:
[0030] (1) Material preparation: The raw materials include by weight: 200 parts of cement, 40 parts of slag, 15 parts of PPR powder, 3 parts of grinding wheel ash, 10 parts of sand, 1 part of thickener, and 300 parts of water;
[0031] (2) Heat the slag, PPR powder and grinding wheel ash to 130°C and stir for 25 minutes;
[0032] (3) Put the mixture of step (2), the thickener, and half of the water into the mixing tank and mix for 10 minutes;
[0033] (4) Put the cement, sand and remaining water into the mixing tank and mix for 20 minutes;
[0034] (5) Transport the uniformly mixed concrete to the site or precast workshop for pouring.
PUM

Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com