Worn-imitated dyeing method of pure cotton black red plaid fabric
A technology of black-red and checkered, which is applied in the field of distressed dyeing of pure cotton black-red woven checkered fabrics. It can solve the problem of uneven overall appearance of distressed depth and shallow layers, and achieve uniform whitening effect, consistent overall appearance, and uniform whiteness. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
specific Embodiment 1
[0024] A method for imitation dyeing of pure cotton black and red plaid fabric, comprising gray yarn→loose winding→chamfering→yarn loading→yarn pretreatment→yarn dyeing→dehydration→whitening→washing, refixing, Dehydration→drying→winding→dyed yarn; among them:
[0025] Among the gray yarns, the yarn specification is: 32S pure cotton yarn;
[0026] In the loose winding, the base yarn is wound from the paper bobbin to the plastic bobbin, the winding speed is 500-600m / min, and the winding density is low, which is convenient for pre-treatment and dyeing in the subsequent process;
[0027] In the described yarn pretreatment, the process prescription is as follows:
[0028]
[0029] The temperature is 90°C, and the time is 40 minutes;
[0030] In the yarn dyeing, the black yarn and the red yarn are respectively dyed, which includes the following steps: bobbin preparation→into the dyeing vat→adding sodium starch→adding alkali agent→hot water washing (85°C, 5min)→ Cold water wash...
specific Embodiment 2
[0043] A method for imitation dyeing of pure cotton black and red plaid fabric, comprising gray yarn→loose winding→chamfering→yarn loading→yarn pretreatment→yarn dyeing→dehydration→whitening→washing, refixing, Dehydration→drying→winding→dyed yarn; among them:
[0044] Among the gray yarns, the yarn specification is: 32S pure cotton yarn;
[0045] In the loose winding, the base yarn is wound from the paper bobbin to the plastic bobbin, the winding speed is 600m / min, and the winding density is low, which is convenient for pre-processing and dyeing in the subsequent process;
[0046] In the described yarn pretreatment, the process prescription is as follows:
[0047]
[0048]
[0049] The temperature is 95°C, and the time is 45 minutes;
[0050] In the yarn dyeing, the black yarn and the red yarn are respectively dyed, which includes the following steps: bobbin preparation→into the dyeing vat→adding sodium starch→adding alkali agent→hot water washing (85°C, 5min)→ Cold w...
specific Embodiment 3
[0063] A method for imitation dyeing of pure cotton black and red plaid fabric, comprising gray yarn→loose winding→chamfering→yarn loading→yarn pretreatment→yarn dyeing→dehydration→whitening→washing, refixing, Dehydration→drying→winding→dyed yarn; among them:
[0064] Among the gray yarns, the yarn specification is: 32S pure cotton yarn;
[0065] In the loose winding, the base yarn is wound from the paper bobbin to the plastic bobbin, the winding speed is 560m / min, and the winding density is low, which is convenient for pre-processing and dyeing in the subsequent process;
[0066] In the described yarn pretreatment, the process prescription is as follows:
[0067]
[0068] The temperature is 92°C, and the time is 43 minutes;
[0069] In the yarn dyeing, the black yarn and the red yarn are respectively dyed, which includes the following steps: bobbin preparation→into the dyeing vat→adding sodium starch→adding alkali agent→hot water washing (85°C, 5min)→ Cold water washing...