Method and system for preparing silver copper oxide composite powder

A technology of silver-copper oxide and composite powder, which is applied in the field of preparation of silver-copper oxide composite powder, which can solve the problems of uneven surface and internal structure of finished materials, poor wettability of oxide particles and substrate interface, and inaccurate contact size, etc. , to achieve large-scale mass production, great theoretical and practical significance, and scientific and reasonable process design

Inactive Publication Date: 2018-10-02
CENT SOUTH UNIV
View PDF0 Cites 5 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0003] In the prior art, the main methods for preparing silver oxide copper electrical contact materials include alloy internal oxidation method and powder metallurgy method, among which, alloy internal oxidation method is a relatively advanced process for preparing electrical contact materials. Simple, low cost, and excellent contact performance, it is widely used at home and abroad, but the surface and internal structure of the finished material prepared by this method are not uniform, and there is a poor oxide layer in the middle, which leads to inaccurate contact dimensions; powder metallurgy method It is one of the main preparation methods of silver metal oxide composite materials. The powder metallurgy method can obtain electrical contact materials with relatively uniform structure and stable performance, but the prepared finished materials have low density, poor processability, high resistivity, Disadvantages such as poor interfacial wettability between oxide particles and the substrate, weak interfacial bonding strength, etc.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Method and system for preparing silver copper oxide composite powder
  • Method and system for preparing silver copper oxide composite powder
  • Method and system for preparing silver copper oxide composite powder

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0065] The embodiment of the present invention prepares silver-copper oxide composite powder according to the above-mentioned preparation method. The specific process is as follows: the molar ratio of copper oxide to silver in the silver-copper oxide composite powder product is preset to be 1:10, and the concentration of silver ions in the precursor solution is set to be 0.1mol / L, weigh 16.99g of silver nitrate and 2.42g of copper nitrate trihydrate according to the amount of 1L precursor solution, add 500ml of deionized water, ultrasonic vibration for 15min to dissolve, and finally constant volume to obtain a clear and transparent precursor solution .

[0066] Subsequently, the temperature of the three constant temperature zones of the vertical resistance furnace was uniformly set to 700 °C, and the precursor solution was passed into the reaction furnace in the form of droplets through an ultrasonic atomization device. The compressed air flow rate was 15 L / min, and the droplet...

Embodiment 2

[0068] The embodiment of the present invention prepares silver-copper oxide composite powder according to the above-mentioned preparation method, the specific process is similar to that of Example 1, the difference is that when preparing the precursor solution, the concentration of silver ions in the precursor solution is controlled to be 0.2mol / L, in addition, high temperature heating The temperature of the three constant temperature zones of the decomposed vertical resistance furnace is uniformly set to 1000°C.

[0069] Such as image 3 Shown is the XRD figure of the silver-copper oxide composite powder prepared by embodiment 1 (3A) and embodiment 2 (3B), as can be seen from the figure, the silver-copper oxide composite powder prepared is mainly Ag phase and CuO phase, and the phases of the powders collected by the three receiving tanks are consistent; at the same time, the silver-copper oxide composite powder collected in each receiving tank is analyzed by scanning electron...

Embodiment 3

[0071] The embodiment of the present invention prepares silver-copper oxide composite powder according to the above preparation method, the specific process is similar to that of Example 2, the difference is that when preparing the precursor solution, the concentration of silver ions in the precursor solution is controlled to 0.05mol / L, and the precursor is added 10V% methanol of the solution was added to the precursor solution. In addition, during the high temperature thermal decomposition process, the droplet flow rate was controlled to be 0.2mL / min.

[0072] The results show that the prepared silver-copper oxide composite powder is mainly Ag phase and CuO phase, and the phases of the powders collected in the three receiving tanks are consistent; at the same time, the silver oxide collected in each receiving tank The scanning electron microscope analysis of the copper composite powder shows that the particle size of the powder in the primary receiving tank is about 3 μm, the ...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
particle diameteraaaaaaaaaa
particle diameteraaaaaaaaaa
particle diameteraaaaaaaaaa
Login to view more

Abstract

The invention discloses a method and system for preparing silver copper oxide composite powder. The preparation method comprises the following steps that 1, silver raw material and copper raw materialare weighed according to the proportion, the sliver raw material and the copper raw material are dissolved to prepare a precursor solution containing silver nitrate and copper nitrate; and 2, an atomization treatment is carried out on the precursor solution to obtain precursor fog drops with the particle size being 0.01-100 [mu]m, and thermal decomposition is carried out on the precursor fog drops at the temperature of 400-1000 DEG C to obtain the silver copper oxide composite powder. The preparation system comprises an atomizing device, a heat treatment device and a cyclone collecting device. The preparation method is characterized in that a proper amount of C1-C4 alcohol is added when the precursor solution is prepared, and therefore the degree of sphericity of the silver copper oxide composite powder can be effectively controlled; a proper amount of ammonia water is added, and therefore the silver copper oxide composite powder with the hollow structure can be prepared; the cyclonecollecting device can be used for effectively grading powder bodies with different particle sizes; and the process design is scientific, the process is continuous, the equipment structure is reasonable, the raw materials are easy to get and low in price, the phase of the reaction product is controllable, the purity is high, the particle size is controllable, large-scale production can be realized,and the application prospect is wide.

Description

technical field [0001] The invention relates to the technical field of preparation of functional powder materials, in particular to a method and system for preparing silver-copper oxide composite powder. Background technique [0002] Silver copper oxide composite powder is a widely used composite material, and its application fields are different with different CuO content. When the copper oxide content is 8-12wt%, it is mainly used as an electrical contact material; the silver copper oxide content is 20wt%. The composite powder can effectively improve the sintering characteristics of the silver powder in the conductive paste; in addition, the silver-copper oxide composite powder can also be used as a catalyst material. At present, silver copper oxide composite powder has attracted much attention due to its relatively stable performance in low-voltage switches, relays and controllers. [0003] In the prior art, the main methods for preparing silver oxide copper electrical c...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): B22F9/30
CPCB22F9/30
Inventor 刘智勇朱银刘志宏李启厚马欢黄辉
Owner CENT SOUTH UNIV
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products