Method for improving scratch resistance of surface of colored inkjet printing paper coating

A color inkjet and printing paper technology, applied in coating, paper coating, papermaking, etc., can solve the problem of easy mechanical scratches on the surface of color inkjet printing paper, and achieve the effect of improving the hardness of the coating

Active Publication Date: 2019-02-19
广东阿博特数码纸业有限公司
View PDF9 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0005] What the present invention aims to solve is the problem that the surface of color inkjet printing paper is easily scratched mechanically during the printing process

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0046] A method for improving the scratch resistance of the coated surface of color inkjet printing paper, comprising the following steps:

[0047] (1) Dry the paper base after the coating process, the drying includes pre-drying and post-drying, the temperature of the pre-drying is 50°C, the temperature of the post-drying is 80°C, the drying method For hot air drying, through electric heating hot air circulation;

[0048] (2) Carry out heat treatment then, the mode of described heat treatment is to dry in the drying room under constant temperature and humidity condition, wherein relative humidity is 30%. Drying room capacity: 36 cubic meters (6*3*2 meters); heating method: electric heating and hot air circulation. The room temperature in the drying room is ~95°C. The time of the heat treatment is 24 hours.

[0049] The paper base undergoes coating and coating processes, and the paper base sequentially includes a coating layer, base paper layer, coating layer and coating lay...

Embodiment 2

[0052] A method for improving the scratch resistance of the coated surface of color inkjet printing paper, comprising the following steps:

[0053] (1) Dry the paper base after the coating process, the drying includes pre-drying and post-drying, the temperature of the pre-drying is 45°C, the temperature of the post-drying is 75°C, the drying method For hot air drying, through electric heating hot air circulation;

[0054] (2) Carry out heat treatment then, the mode of described heat treatment is to dry in the drying room under constant temperature and humidity condition, wherein relative humidity is 35%. Drying room capacity: 36 cubic meters (6*3*2 meters); heating method: electric heating and hot air circulation. The temperature of the heat treatment is 90° C., and the time of the heat treatment is 22 hours.

[0055] The paper base undergoes coating and coating processes, and the paper base sequentially includes a coating layer, base paper layer, coating layer and coating l...

Embodiment 3

[0058] A method for improving the scratch resistance of the coated surface of color inkjet printing paper, comprising the following steps:

[0059](1) Dry the paper base after the coating process, the drying includes pre-drying and post-drying, the temperature of the pre-drying is 55°C, the temperature of the post-drying is 80°C, the drying method For hot air drying, through electric heating hot air circulation;

[0060] (2) Carry out heat treatment then, the mode of described heat treatment is to dry in the drying room under constant temperature and humidity condition, wherein relative humidity is 30%. Drying room capacity: 36 cubic meters (6*3*2 meters); heating method: electric heating and hot air circulation. The temperature of the heat treatment is 95° C., and the time of the heat treatment is 26 hours.

[0061] The paper base undergoes coating and coating processes, and the paper base sequentially includes a coating layer, base paper layer, coating layer and coating la...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses a method for improving the scratch resistance of the surface of a colored inkjet printing paper coating. The method comprises the following steps of (1) drying a paper base after treatment based on a coating process; (2) then, performing heat treatment. The method only requires little investment, can effectively improve the hardness and scratch resistance of the coating through batched heat treatment of the product, and can be well implemented in terms of technology and operation, and the purpose of improvement can be achieved at last.

Description

technical field [0001] The invention relates to paper printing technology, in particular to a method for improving the anti-scratch performance of the coating surface of color inkjet printing paper. Background technique [0002] Color inkjet printing paper is a high-end image output product, which has very high requirements on the surface performance of the paper. Especially with the rapid changes of color inkjet printing equipment and continuous innovation of technology, the requirements for image printing media are becoming more and more stringent, especially for the performance and adaptability of color inkjet printing paper. [0003] Due to the particularity of the production process of color inkjet printing paper and the coating formula, the emphasis is on ink absorption, quick drying, color reducibility and color fastness, etc., resulting in a color carrier, that is, a weak embodiment of the hardness of the coating. , that is, the scratch resistance of the coating wil...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): D21H25/06D21H19/82D21H19/84
CPCD21H19/82D21H19/84D21H25/06
Inventor 周国苗
Owner 广东阿博特数码纸业有限公司