Embodiment 1
[0028] The production process of antibacterial fabric comprises the following steps:
[0029] (1) 8 parts by weight of water-based polyurethane emulsion, 0.9 parts by weight of carbon nanotubes, 0.4 parts by weight of surfactant, 0.5 parts by weight of sodium polyacrylate, 0.3 parts by weight of coupling agent, and 0.6 parts by weight of antimicrobial agent are added to 90 parts by weight to remove Stir in deionized water at a speed of 300r / min for 20min and mix evenly to obtain a finishing solution;
[0030] (2) Immerse the fabric in the finishing solution at a bath ratio of 1:40 (g / mL) for 60 minutes, the dipping temperature is 40°C, one dipping and one rolling, the excess rate is 75%, the fabric is taken out, and pre-baked at 95°C After 4 minutes, dry at 40°C for 30 hours to obtain an antibacterial fabric.
[0031] The surfactant is dodecyltrimethylammonium chloride.
[0032] The antibacterial agent is chitosan biguanide hydrochloride.
[0033] The coupling agent is 3-(m...
Embodiment 2
[0038] The production process of antibacterial fabric comprises the following steps:
[0039] (1) 8 parts by weight of water-based polyurethane emulsion, 0.9 parts by weight of modified carbon nanotubes, 0.4 parts by weight of surfactant, 0.5 parts by weight of sodium polyacrylate, 0.3 parts by weight of coupling agent, and 0.6 parts by weight of antibacterial agent are added to 90 parts by weight in turn One part of deionized water was stirred at a speed of 300r / min for 20min and mixed evenly to obtain a finishing solution;
[0040] (2) Immerse the fabric in the finishing solution at a bath ratio of 1:40 (g / mL) for 60 minutes, the dipping temperature is 40°C, one dipping and one rolling, the excess rate is 75%, the fabric is taken out, and pre-baked at 95°C After 4 minutes, dry at 40°C for 30 hours to obtain an antibacterial fabric.
[0041] The surfactant is dodecyltrimethylammonium chloride.
[0042] The antibacterial agent is chitosan biguanide hydrochloride.
[0043] T...
Embodiment 3
[0049] The production process of antibacterial fabric comprises the following steps:
[0050] (1) 8 parts by weight of water-based polyurethane emulsion, 0.9 parts by weight of modified carbon nanotubes, 0.4 parts by weight of surfactant, 0.5 parts by weight of sodium polyacrylate, 0.3 parts by weight of coupling agent, and 0.6 parts by weight of antibacterial agent are added to 90 parts by weight in turn One part of deionized water was stirred at a speed of 300r / min for 20min and mixed evenly to obtain a finishing solution;
[0051] (2) Immerse the fabric in the finishing solution at a bath ratio of 1:40 (g / mL) for 60 minutes, the dipping temperature is 40°C, one dipping and one rolling, the excess rate is 75%, the fabric is taken out, and pre-baked at 95°C After 4 minutes, dry at 40°C for 30 hours to obtain an antibacterial fabric.
[0052] The surfactant is dodecyltrimethylammonium chloride.
[0053] The antibacterial agent is chitosan biguanide hydrochloride.
[0054] T...