Wood treatment process
A technology of wood treatment and treatment process, applied in wood treatment, wood treatment details, wood processing equipment, etc., can solve the problems of uneven color of surface wood, color difference and color change of early wood and late wood of heartwood, and achieve good bleaching effect , meet the requirements, optimize the effect of bleaching process parameters
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] A kind of wood processing technology, described processing technology comprises the steps:
[0020] a. Soak the wood with dilute sulfuric acid solution for 1h;
[0021] b. Wash the wood with water;
[0022] c. Soak the wood with sodium hydroxide solution for 30 minutes;
[0023] d. Wash the wood with water;
[0024] e. Treatment of wood with bleaching agent;
[0025] f. Wash wood with water and dry.
[0026] Wherein, the concentration of the dilute sulfuric acid solution is 3%.
[0027] Wherein, the concentration of the sodium hydroxide solution is 0.3%.
[0028] Wherein, the bleaching agent includes the following components in weight percentage: 50% hydrogen peroxide with a concentration of 30%, 10% ammonia water with a concentration of 25%, 1% sodium bicarbonate, 2% ammonium fluorosilicate, and the balance is water.
Embodiment 2
[0030] A kind of wood processing technology, described processing technology comprises the steps:
[0031] a. Soak the wood with dilute sulfuric acid solution for 2 hours;
[0032] b. Wash the wood with water;
[0033] c. Soak the wood with sodium hydroxide solution for 100 minutes;
[0034] d. Wash the wood with water;
[0035] e. Treatment of wood with bleaching agent;
[0036] f. Wash wood with water and dry.
[0037] Wherein, the concentration of the dilute sulfuric acid solution is 1%.
[0038] Wherein, the concentration of the sodium hydroxide solution is 0.1%.
[0039] Wherein, the bleaching agent includes the following components in weight percentage: 70% hydrogen peroxide with a concentration of 30%, 15% ammonia water with a concentration of 25%, 0.1% sodium bicarbonate, 0.1% ammonium fluorosilicate, and the balance is water.
Embodiment 3
[0041] A kind of wood processing technology, described processing technology comprises the steps:
[0042] a. Soak the wood with dilute sulfuric acid solution for 1h;
[0043] b. Wash the wood with water;
[0044] c. Soak the wood in sodium hydroxide solution for 80 minutes;
[0045] d. Wash the wood with water;
[0046] e. Treatment of wood with bleaching agent;
[0047] f. Wash wood with water and dry.
[0048] Wherein, the concentration of the dilute sulfuric acid solution is 2%.
[0049] Wherein, the concentration of the sodium hydroxide solution is 0.2%.
[0050] Wherein, the bleaching agent includes the following components in weight percentage: 55% hydrogen peroxide with a concentration of 30%, 13% ammonia water with a concentration of 25%, 05% sodium bicarbonate, 1.2% ammonium fluorosilicate, and the balance is water.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com