Method for masking holes in element and treating element
An element and masking technology, applied in the field of masking holes in elements, can solve the problems of low efficiency, time-consuming and labor-intensive
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
example
[0043] Using acrylic epoxy as the masking material, place the Figure 4 The blade to be repaired with a ceramic thermal barrier coating on the surface shown is immersed in the electrophoretic solution containing acrylic epoxy resin particles, used as the cathode, and the other blade is used as the anode, and a voltage of 10-300V is applied to the cathode and the anode for 1~ 30 minutes of electrophoretic deposition, during which particles of acrylic epoxy resin enter the cooling holes of the blade to be repaired. After the electrophoretic deposition is completed, the blade filled with acrylic epoxy resin in the cooling hole is baked at a temperature of about 160° C. for about 20 minutes, so that the acrylic epoxy resin in the cooling hole is formed denser and firmer. structure, so that the cooling hole can be well covered (such as Figure 5 shown). Then sandblasting is performed on the blade with the cooling holes masked to remove the thermal barrier coating on the surface o...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More 