Angstrom silver, Angstrom silver gel for external use, preparation method and application
A gel and Amy technology, applied in the field of medicine, can solve problems such as slow wound healing, scarring, affecting the quality of life of patients and personal self-confidence
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0052] A kind of angstrom silver of the present invention, its preparation method comprises the following steps:
[0053] (1) Fill the explosion chamber with inert gas argon to keep the air pressure in the explosion chamber at 1×10 6 Pa, and stabilize the working temperature at 8-12°C.
[0054] (2) Continuously push a silver wire with a diameter of 0.5mm and a length of 8-12cm into the explosion chamber. When the silver wire contacts the positive plate, a high voltage of 25kV is generated, causing the silver wire to explode and instantly evaporate the silver wire into silver. vapor plasma.
[0055] (3) The silver vapor accompanied by argon gas is pumped into the quenching chamber whose temperature is set at 0-4° C., and the silver vapor solidifies rapidly when it is cold and forms silver particles.
[0056] (4) The silver particles are dispersed by high-intensity ultrasonic waves (ultrasonic power is 15KW, frequency is 15KHz), and the dispersed silver particles are sucked to...
Embodiment 2
[0060] A kind of angstrom silver external use gel of the present invention, comprises 1.0g / L the angstrom grade elemental silver powder, the carbomer 934P of 9.8g / L, the triethanolamine of 5g / L, the high-purity bismuth of 984.2g / L distilled water.
[0061] Its preparation method comprises the following steps:
[0062] (1) Get the angstrom silver in Example 1 and add it in double-distilled water, use an ultrasonic oscillator to carry out dispersion treatment, control the ultrasonic power to 5KW, the frequency is 40KHz, and the dispersion time is 60s; the concentration obtained is 1.0g / L angstrom silver Dispersions.
[0063] (2) Add Carbomer 934P to the angstrom silver dispersion, and then use a magnetic rotor high-speed stirrer with a stirring speed of 2000 rpm to cut the angstrom silver solution until it is completely clarified to obtain a mixed solution. The concentration of Carbomer 934P in the mixed solution was 9.8g / L.
[0064] (3) Add triethanolamine to the mixed solut...
Embodiment 3
[0069] The application of the angstrom silver external gel of a kind of embodiment 2 in the preparation antibacterial preparation, its application method is:
[0070] (1) Grouping:
[0071] Blank group (Blank): double distilled water.
[0072] Empty gel group (Vehicle): including 9.8g / L carbomer 934P, 5g / L triethanolamine, and 984.2g / L double distilled water.
[0073] Nano silver gel group (AgNPs gel): Silki gel, which uses 1.0g / L nano-scale elemental silver powder.
[0074] Angstrom silver topical gel group ( gel): 1.0g / L angstrom level elemental silver powder, 9.8g / L carbomer 934P, 5g / L triethanolamine, 984.2g / L double distilled water.
[0075] (2) After the solutions of the above groups were made into gels, the circular paper pieces with a diameter of 6 mm were placed in each group of intervention agents and soaked for 12 hours. Place on the coated bacteria MH plate. Bacterial species: Streptococcus pyogenes (ATCC19615), Pseudomonas aeruginosa (ATCC 27853), Escherichi...
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
length | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com