Device and method for measuring moisture diffusion coefficient of cement-based material
A technology of cement-based materials and diffusion coefficients, which is applied in the direction of measuring devices, suspension and porous material analysis, and analytical materials. Short, mature equipment, the effect of reducing time
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0046] Embodiment 1: as Figure 1-7 As shown, a device for measuring moisture diffusion coefficient of cement-based materials, including: 1. mold; 2. embedded pipe; 3. temperature and humidity sensor; 4. portable data analyzer; 5. mold base; 6. embedded pipe clamp ;7, inserting plate; 8, bottom surface of mold; 9, side of mold; 10, side of mold; 11, side of mold; 12, side of mold; 13, mold handle; 14, sealant between temperature and humidity sensor and embedded pipe Sealing treatment; 15. Anti-seepage slurry material for embedded pipes; 16. Gap reserved at the end of embedded pipes; 17. Sealing treatment for non-dry surfaces of concrete specimens; 18. The gap between the temperature and humidity sensor and the embedded pipe Sealing ring; 19, computer; 20, card slot; 21, the reserved bolt hole on the side (12); 22, the reserved semicircular hole on the side (12); 23, the circular hole in the center of the mold bottom surface; 24, the plug Reserved bolt holes on the plate (7); ...
Embodiment 2
[0067] Embodiment 2: a kind of measuring method of cement-based material moisture diffusion coefficient measuring device, adopt described measuring device, select C30 concrete for use, concrete mix ratio is as follows:
[0068] Cement: water: sand: stone: fly ash = 240:186:750:1150:60
[0069] Include the following steps:
[0070] S1. The height of the sides of the mold (9), (10), and (11) is 50 mm. Place the three embedded pipes (2) on the mold base (5). The embedded depths of the three embedded pipes (2) are respectively 20mm, 60mm, 100mm, the pre-embedded pipe (2) is fixed by the pre-embedded pipe clamp (6), and the gap (16) at the end of the pre-embedded pipe is 2mm wide;
[0071] S2. After fixing the 3 pre-embedded pipes (2), insert the inserting plate (7) into the base (5), and connect with the side (12) with 2 screws to further fix the pre-embedded pipe (2) and the inserting plate ( 7);
[0072] S3, block the round hole (23) on the bottom surface (8) with a film or p...
PUM
Property | Measurement | Unit |
---|---|---|
Gap width | aaaaa | aaaaa |
Height | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com