Method for improving moist feeling of decorative wood material
A technology of wood decoration and treatment method, which is applied to wood processing utensils, treatment details of cork stoppers, and manufacturing tools, etc. The effect of luster is pleasing to the eye, improves hand feel, and enhances high-end feeling
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0008] Moisturizing treatment after dyeing
[0009] After natural wood decoration materials are dyed, add non-silicon and non-ionic softener in the washing tank, which will not interact with dyes and additives, and make the natural wood decoration materials feel comfortable and oily through adsorption. Non-silicon non-ionic softener such as Tianjin Da-Qi Fine Chemical Co., Ltd.'s softener N-100, Qingdao Dayuan Chemical Co., Ltd.'s softener 9L, American Gaobao Chemical Group's softener FC, or other non-silicon non-ionic softeners . The specific process is as follows:
[0010] Wood shavings→boiling and bleaching→staining→(washing)→moisturizing treatment [softener N-100 1-8% (relative to the weight of wood shavings), bath ratio about 1:10, temperature about 40°C, time 10-30 minutes ].
Embodiment 2
[0012] Moisturizing treatment after dyeing
[0013] After the natural wood decoration material is dyed, add non-silicon and non-ionic softener in the washing tank, and make the natural wood decoration material feel comfortable and oily through adsorption. The specific process is as follows:
[0014] Wood shavings→boiling and bleaching→staining→(washing)→moisturizing treatment [softener 9L 1-8% (relative to the weight of wood shavings), bath ratio about 1:10, temperature about 40°C, time 10-30 minutes].
Embodiment 3
[0016] Moisturizing treatment after dyeing
[0017] After the natural wood decoration material is dyed, add non-silicon and non-ionic softener in the washing tank, and make the natural wood decoration material feel comfortable and oily through adsorption. The specific process is as follows:
[0018] Wood shavings→boiling and bleaching→staining→(washing)→moisturizing treatment [softener FC 1-8% (relative to the weight of wood shavings), bath ratio about 1:10, temperature about 40°C, time 10-30 minutes].
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com