[0012] The optimum raw material ratio that embodiment adopts is: (weight ratio)
[0014] Dibutyl phthalate 25%
[0015] Xylene 35%
[0016] The production sequence of oleic acid 5% is:
[0017] 1. Soaking: Soak cadmium oxide in dibutyl phthalate-2-carboxylate.
[0018] 2. Grinding: The soaked mixture is repeatedly ground with a three-roll mill until it becomes a paste.
[0019] 3. Mixing: Mix and stir the paste with xylene and oleic acid to adjust to an appropriate concentration.
[0020] 4. Filling and core making: the finished product of process 3 is filled in the core tube of the ballpoint pen core with the pen core filling machine, and the grease seal and the nib installation are carried out.
[0021] 5. Pen making: put the prepared pen core into the pen case, and it is ready.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com