Light-diffusing film
A light-diffusing and thin-film technology, applied in the field of light-diffusing thin films, can solve problems such as difficult to achieve high brightness and shielding
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0039] Step 1: Formation of Light Diffusing Layer
[0040] The light-diffusing layer composition, comprising the composition shown in Table 1 below, was coated on one surface of a highly transparent polyester film (XG533-100um, Toray Saehan Inc.) as a substrate, and then coated on It was dried at 110° C. for 60 seconds to form a 30 μm thick light-diffusing layer.
[0041] combination
Types of
amount (g)
resin
A-811 (Aekyung Chemical Co. Ltd.)
30
particles
PMMA (specific surface area 0.9)
30
MEK
40
Total
100
[0042] Step 2: Formation of anti-adhesion layer
[0043] The anti-blocking layer composition, comprising the composition shown in the following Table 2, was coated on the other surface of the substrate having the light-diffusing layer prepared in step 1, and then dried at 110° C. for 40 seconds , forming a 5 μm thick anti-blocking layer, thereby preparing the final light-...
PUM
| Property | Measurement | Unit |
|---|---|---|
| diameter | aaaaa | aaaaa |
| thickness | aaaaa | aaaaa |
| thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com