Adhesion force promoter composition, preparation method and application thereof
A technology of adhesion promoter and composition, applied in application, household appliances, ink and other directions, can solve the problems of increasing corona equipment, solvent combustion, adverse effects of ink system stability, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0042] Another aspect of the present application relates to the preparation method of above-mentioned adhesion promoter composition, it comprises the following steps:
[0043] (1) mix the polyurethane resin in the diluent evenly;
[0044] (2) adding organic chelate and mixing; and
[0045] (3) Add special surfactant and mix well.
[0046] In the above step (1), medium-speed stirring is preferably used.
[0047] In the above step (2), high-speed stirring is preferably used, and the reaction is allowed to stand for 1 hour after uniform mixing.
[0048] In the above step (3), high-speed stirring is preferably used.
[0049] Another aspect of the present application relates to the use of the above-mentioned adhesion promoter composition in the production of security lines, including: for pre-press treatment, interlayer use or as an ink additive.
[0050] The pre-press treatment is to print or coat the adhesion promoter composition of the present application or its dilution on ...
Embodiment 1
[0071] 20wt.% PU200
[0072] 5wt.% IAM
[0073] 0.1wt.% FSJ:SMA=5:1
[0074] 74.9wt.% Butanone
[0075] How to use: Use as an interlayer coating
[0076] Adhesion fastness: the ink fastness is grade 2 before using this adhesion promoter, and grade 4~5 after using it.
Embodiment 2
[0078] 25wt.% U-347
[0079] 10wt.% IAM
[0080] 0.5wt.% FSJ:SMA=10:1
[0081] 64.5wt.% ethyl acetate
[0082] Method of use: used as an ink additive
[0083] Adhesion fastness: the ink fastness is grade 1-2 before using this adhesion promoter, and grade 4-5 after using it.
[0084] At the same time, it improves the inferiority of the ink such as floating color and blooming. Before using this adhesion promoter, the product waste caused by ink floating and blooming is 2%, and it is reduced to less than 0.1% after use.
PUM
| Property | Measurement | Unit |
|---|---|---|
| surface tension | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information