Method for producing bamboo charcoal slow-resilience foam material
A production method and technology of foam materials, applied in the production field of bamboo charcoal slow rebound foam materials, can solve the problems of slow rebound foam without specific adsorption, health care function, unfavorable health and environmental protection, nourishing bacteria, etc., and achieve easy operation , low cost, good adsorption effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment
[0014] Put the truncated bamboo or bamboo processing leftovers into a carbonization furnace and burn them at a temperature of about 700°C for 2 hours, cool them down to room temperature naturally, take them out, crush them and sieve them, and collect 200-320 mesh (0.071mm- 0.045mm) bamboo charcoal, washed with water and dried to dryness for later use.
[0015] Preparation of composite washed dry powdered bamboo charcoal with the prepared washed dry powdered bamboo charcoal
[0016] Uniform dispersant 60NS is mixed in a ratio of 1:0.05 by weight for later use.
[0017] Add the composite washed dry powdered bamboo charcoal, polyether polyol, water, glycerin, surfactant, and catalyst into the mixing tank according to the ratio in Table 1. After stirring evenly, keep the material temperature at 24-28°C, and then Then add Cosmonate T-80 according to the ratio in Table 1, stir rapidly for 7 to 10 seconds, and then quickly follow the conventional operating procedures.
[0018] The ...