Water-based colorful imitation marble paint
A marble-like paint and colorful technology, applied in the field of paint, can solve the problems of difficult industrial production and the inability to guarantee the stability of paint particles
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0039] (1), preparation of color particle components (monochrome): weigh 35 parts of 7104 acrylic emulsion, 25 parts of deionized water, additives (including 0.3 parts of cellulose, 0.6 parts of dispersant, 3 parts of antifreeze) ), 0.3 parts of xanthan gum, 30 parts of pigments and fillers, under low-speed (400r / min-500r / min) stirring, add auxiliary agents and xanthan gum composed of dispersant, cellulose, antifreeze to water, and stir for 5 minutes -10min, adjust the speed to medium speed (600r / min-800r / min), slowly and uniformly add pigments and fillers, disperse at high speed (1200r / min-1500r / min) for 45 minutes, grind to a fineness below 45μm with a grinder, add The metered 7104 acrylic acid emulsion was stirred evenly to obtain a single-color particle base material, which was ready for use;
[0040] (2), preparation of protective colloid: take by weight 0.8 parts of suspending agent, 30 parts of deionized water, 1 part of ionic compound, 60 parts of 7104 acrylic acid emu...
Embodiment 2
[0044]1. Preparation of color particle components (single color): weigh 40 parts of KD8 emulsion, 20 parts of deionized water, additives (including 0.2 parts of cellulose, 1.0 parts of dispersant, 3 parts of antifreeze), yellow 0.5 parts of raw gum, 35 parts of pigments and fillers, under low speed (400r / min-500r / min) stirring, add additives consisting of dispersant, cellulose, antifreeze agent and xanthan gum into the water, stir for 5min-10min, Adjust the speed to medium speed (600r / min-800r / min), add pigments and fillers at a slow and uniform speed, disperse at high speed (1200r / min-1500r / min) for 45 minutes, grind to a fineness below 45μm with a grinder, and add metered KD8 emulsion, stir evenly to obtain monochromatic particle base material, stand-by;
[0045] 2. Preparation of protective colloid: weigh 1.5 parts of suspending agent, 25 parts of deionized water, 1.5 parts of ionic compound, 70 parts of 7104 acrylic emulsion and 4.5 parts of functional dispersant. During p...
Embodiment 3
[0049] a. Preparation of color particle components (single color): weigh 45 parts of 996D silicone acrylic emulsion, 25 parts of deionized water, and additives (including 0.3 parts of cellulose, 0.6 parts of dispersant, and 3 parts of antifreeze) , 0.5 parts of xanthan gum, 25 parts of pigments and fillers, under low-speed (400r / min-500r / min) stirring, add additives and xanthan gum composed of dispersant, cellulose, antifreeze to the water, stir for 5min- 10min, adjust the speed to medium speed (600r / min-800r / min), slowly and uniformly add pigments and fillers, disperse at high speed (1200r / min-1500r / min) for 45 minutes, grind with a grinder to a fineness below 45μm, add and measure The 996D silicon-acrylic emulsion that has been passed is stirred evenly to obtain a single-color particle base material, which is set aside;
[0050] b. Prepare protective colloid: weigh 1.2 parts of suspending agent, 30 parts of deionized water, 1 part of ionic compound, 65 parts of 7104 acrylic ...