A kind of imitation marble, a kind of colorful technology, applied in the field of preparation of colorful imitation marble paint, can solve the problems of inability to guarantee the stability of particles, affect the progress of the project, difficult industrial production and other problems, achieve high stability, good self-cleaning, good Stretch effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] A kind of preparation method of colorful imitation marble paint, prepares the raw material of weight portion: the pigment of 6 kinds of colors and lusters, the pigment of every kind of colors and lusters is modulated into 100kg with latex paint, totally 600kg, takes by weighing 240kg of toning emulsion, 141kg of deionized water, making Granular emulsion 90kg, 6kg defoamer; Prepare according to the following steps:
[0016] a) Mix 40kg of toning emulsion with 16kg of deionized water and stir evenly;
[0017] b) Add one type of monochrome latex paint and stir for 25 minutes;
[0018] c) Then add 15kg granulated emulsion and 7.5kg deionized water, and stir for 10min; add defoamer;
[0019] d) Prepare the remaining 5 kinds of monochrome latex paints according to the above steps a-c, mix these 6 kinds of prepared monochrome latex paints, and stir for 10 minutes.
Embodiment 2
[0021] A kind of preparation method of colorful imitation marble paint, prepare the raw material of weight portion: the pigment of 7 kinds of colors and luster, the pigment of every kind of color and luster is modulated into 100kg with latex paint, totally 700kg, takes by weighing 420kg of toning emulsion, 255.5kg of deionized water, Granulated emulsion 175kg, 7kg defoamer; prepared according to the following steps:
[0022] a) Mix 60kg of toning emulsion with 24kg of deionized water and stir evenly;
[0023] b) Add one type of monochromatic latex paint and stir for 35 minutes;
[0024] c) Then add 25kg granulated emulsion and 12.5kg deionized water, and stir for 15min; add defoamer;
[0025] d) Prepare the remaining 6 kinds of single-color latex paints according to the above steps a-c, mix these 7 kinds of prepared single-color latex paints, and stir for 15 minutes.
Embodiment 3
[0027] A kind of preparation method of colorful imitation marble paint, prepares the raw material of weight portion: the pigment of 8 kinds of colors and lusters, the pigment of every kind of colors and lusters is modulated into 100kg with latex paint, altogether 800kg, takes by weighing 400kg of toner emulsion, 240kg of deionized water, makes Granular emulsion 160kg, 16kg defoamer; prepare according to the following steps:
[0028] a) Mix 50kg of toner emulsion with 20kg of deionized water and stir evenly;
[0029] b) Add one type of monochrome latex paint and stir for 30 minutes;
[0030] c) Then add 20kg granulated emulsion and 10kg deionized water, and stir for 12min; add defoamer;
[0031] d) Prepare the remaining 7 kinds of single-color latex paints according to the above steps a-c, mix these 8 kinds of prepared single-color latex paints, and stir for 12 minutes.