[0011] Add 5 parts of leveling agent to every 100 parts of pigment-containing mixed paint. The formula of leveling agent is 50-60 parts of clay, 10-20 parts of calcium carbonate, 15-20 parts of styrene-butadiene rubber, and 1-2 parts of tetrasodium pyrophosphate. , 8-10 parts of fluorine-containing surfactant. Preferable: 60 parts of pottery clay, 20 parts of calcium carbonate, 20 parts of styrene-butadiene rubber, 1 part of tetrasodium pyrophosphate, and 8 parts of fluorine-containing surfactant. The added paint has no orange peel phenomenon after spraying and is suitable for high-speed roller coating.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com