Method for increasing adhesion between a security element and a fibrous sheet material
A technology of anti-counterfeiting components and fiber materials, applied in the direction of fiber raw material processing, non-fiber pulp addition, chemical instruments and methods, etc., can solve problems such as adverse economic effects, and achieve the effect of increasing design options and firm thickness
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment Construction
[0026] Activatable adhesive films adhered to security strips or security tapes, once activated, serve to more securely fasten these strips to the sheet-like fibrous material. After activation, the membrane softens and penetrates into the surrounding sheet-like fibrous material, forming a mechanical as well as a chemical bond with the sheet-like material. Documents made from these sheet-like fiber materials exhibit enhanced durability.
[0027] As mentioned above, the method of the present invention to enhance the adhesion between the security element and the sheet-like fibrous material includes:
[0028] adhering one or more activatable adhesive films to at least one surface of the security element to form a laminated structure;
[0029] (i) introducing the laminated structure onto or into the forming fibrous web in the wet end of a fourdrinier or twin wire papermaking machine, or (ii) combining the laminated structure with the fibrous web forming drum in a cylinder Contact,...
PUM
| Property | Measurement | Unit |
|---|---|---|
| thickness | aaaaa | aaaaa |
| width | aaaaa | aaaaa |
| thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More 