Embodiment 120
[0043] Embodiment 120% pymetrozine suspension concentrate
[0044] Get 20g of pymetrozine raw powder, 15g of dispersant carboxylate terpolymer, 2g of thickener xanthan gum XG, 10g of stabilizer phenyl glycidyl ether, silicone defoamer silicone oil (dimethyl silicone oil) 6g, 4g of osmotic agent antifreeze propylene glycol, appropriate amount of pH regulator to make the pH value of the suspending agent 8, add deionized water to 100g. After mixing evenly, ball mill in a ball mill for 2 to 3 hours to make the particle size below 3um.
[0045] Dispersant carboxylate terpolymer preparation method is:
[0046] a) Add 50g of water, 50g of methanol and 6g of chain transfer agent dodecylmercaptan into the reaction flask, stir and heat to 60-100°C;
[0047] b) Add 10g styrene, 70g methacrylic acid, 20g hydroxypropyl acrylate and initiator potassium persulfate solution dropwise, dropwise within 1 to 5 hours, then keep warm for 2 to 10 hours; the amount of potassium persulfate is 6g , ...
Embodiment 225
[0052] Embodiment 225% pymetrozine suspension concentrate
[0053] Each component by weight is 25g of pymetrozine raw powder, 15g of dispersant carboxylate terpolymer, 3g of thickener hydroxymethyl cellulose, 2.5g of stabilizer butyl glycidyl ether, defoamer ten Trialkanoic acid 1g, antifreeze agent glycerin 3g, pH adjuster appropriate amount to make the pH value of the suspending agent 7, add deionized water to 100g. After mixing evenly, ball mill in a ball mill for 2 to 3 hours to make the particle size below 3um. The preparation method of carboxylate terpolymer dispersant is the same as in Example 1.
[0054] The suspending agent prepared by the formula has a suspension rate of 97.80%, good dispersibility and an average particle diameter of 2.3um.
Embodiment 325
[0055] Embodiment 325% pymetrozine suspension concentrate
[0056] Each component by weight is 25g of pymetrozine raw powder, 10g of dispersant carboxylate terpolymer, 3g of thickener methyl cellulose, 2.5% of stabilizer phenyl glycidyl ether, defoamer saturated fatty acid Pentadecanoic acid 1g, antifreeze agent glycerin 3%, pH adjuster appropriate amount to make the pH value of the suspending agent 7, add deionized water to 100g. After mixing evenly, ball mill in a ball mill for 2 to 3 hours to make the particle size below 3um.
[0057] Dispersant carboxylate terpolymer preparation method is:
[0058] a) Add 120g of water, 80g of ethanol and 10g of chain transfer agent sodium formate into the reaction flask, stir and heat to 60-100°C;
[0059] b) 20g styrene, 50g methacrylic acid, 30g hydroxypropyl acrylate and initiator hydrogen peroxide-ferrous salt solution are added dropwise, and the addition is completed within 1 to 5 hours, and then the insulation reaction is carried ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com