Wood drying method

A wood drying and drying technology, applied in the direction of drying solid materials, method combination to dry solid materials, drying, etc., can solve problems such as increase in production cost, and achieve the effects of avoiding waste, stable product quality, and obvious energy saving.

Inactive Publication Date: 2014-06-11
广元亿明生物科技有限公司
View PDF7 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

If the temperature is too high in the low temperature preheating stage, it will cause an increase in production costs

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0036] Pressure 0.3mpa, preheat at 35°C, humidity 33%; pressurize to 0.4mpa, temperature rise to 50.5°C, control humidity; ventilate and dry, pressure at 0.4mpa, control temperature and humidity, and keep for 72 hours; pressure 0.3mpa, temperature 55.5°C, humidity 53.5%, keep it for 4 hours; pressure 0.4mpa, secondary drying for 48-72 hours; pressure 0.3mpa, temperature and humidity rise to 62.5°C and 54% for 3 hours, then reduce the temperature and humidity, and the surface is dry . After testing, the 30-day damage value is 0.6.

Embodiment 2

[0038] Pressure 0.8 mpa, preheat at 37°C, humidity 35%; pressure 0.8mpa, temperature rises to 49.5°C, control humidity; ventilate and dry, pressure 0.8mpa, control temperature and humidity, and keep for 72 hours; pressure 0.6mpa, temperature 56.5 ℃, humidity 54.5%, keep for 6 hours; pressure 0.6mpa, secondary drying for 72 hours; pressure 0.6mpa, temperature and humidity rise to 63.5℃ and 66% for 3 hours, then lower the temperature and humidity, and the surface is dry. After testing, the 30-day damage value is 0.58.

Embodiment 3

[0040] Pressure 0.5 mpa, preheat at 36°C, humidity 34%; pressure 0.5mpa, temperature rise to 50°C, control humidity; ventilate and dry, pressure 0.5mpa, control temperature and humidity, and keep for 72 hours; pressure 0.4mpa, temperature 56 ℃, humidity 54%, keep for 5 hours; pressure 0.5mpa, secondary drying for 54 hours; pressure 0.4mpa, temperature and humidity rise to 63℃ and 60% for 3 hours, then lower the temperature and humidity, and the surface is dry. After testing, the 30-day damage value is 0.57.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses a wood drying method, which comprises the following steps: 1 low temperature preheating, 2 preliminary-stage processing, 3 ventilating and drying, 4 middle-stage processing, 5 secondary drying, 6 final processing, 7 lowering humiture and surface drying. The technical scheme of the wood drying method well resolves the problem of wood mustiness caused by over low temperature in the low temperature preheating stage or the preliminary processing stage, thereby being suitable for industrial production.

Description

technical field [0001] The invention relates to a method for treating wood, in particular to a method for preventing mildew, and belongs to the field of wood processing. Background technique [0002] Pure solid wood furniture has natural color and beautiful pattern, stable and durable structure, and it is also the most ideal furniture in history, which is deeply loved by people. Therefore, wood is the most ideal material for making high-end furniture in the world. [0003] However, there are also unsatisfactory disadvantages in that natural wood is directly used to make furniture only through ordinary drying treatment: as the floor of the kitchen, bathroom or north-facing room, it is easy to mold and rot in a long-term humid environment. This is an unsolvable problem in solid wood furniture itself, and it is also the most troublesome place for many solid wood furniture manufacturers. [0004] There are many reasons for wood mold. The common mold in this field is mainly caus...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Patents(China)
IPC IPC(8): F26B7/00
Inventor 赵德勇陈洪义柯昌林
Owner 广元亿明生物科技有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products