A production method and slow-release urea technology are applied in fertilizer mixtures, fertilization devices, applications, etc., and can solve problems such as low nutrient utilization rate, land, environmental impact, resource waste, etc., and achieve low operating costs, elimination of excessive waste, The effect of slowing down the release speed
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0025] When making 1000 kg of the present invention, 30 kg of attapulgite powder, 1 kg of polyacrylamide, 1 kg of quartz stone powder and 968 kg of molten urea solution.
[0026] 1. Put 30 kg of attapulgite powder, 1 kg of polyacrylamide, and 1 kg of quartz stone powder into the slow-release agent feeding device 1 and mix them through the metering belt 2, slow-release agent tank 4 and powder pump 5 into the urea solution tank 6 Inside;
[0027] Two, 968 kilograms of molten urea solutions that come from evaporation system 8 in urea production are 968 kilograms of molten urea solutions that are more than 99.5% and enter in the urea solution tank 6 through the pipeline that flow meter 9 is installed;
[0028] Three, the sustained-release agent mixed in step 1 and the molten urea solution in step 2 are placed on the urea solution tank 6 and uniformly mixed, and the pressure of the urea solution tank 6 is 0.5MPa, and the temperature is 135°C;
[0029] 4. Put the mixed mixture in s...
Embodiment 2
[0032] When making 2000 kg of the present invention, 120 kg of attapulgite powder, 10 kg of polyacrylamide, 10 kg of quartz stone powder and 10 kg of molten urea solution.
[0033] 1. Put 120 kg of attapulgite powder, 10 kg of polyacrylamide, and 10 kg of quartz stone powder into the slow-release agent feeding device 1 and mix them into the urea solution tank 6 through the metering belt 2, the slow-release agent tank 4 and the powder pump 5 Inside;
[0034] Two, 1860 kilograms of molten urea solution that the concentration that comes from evaporation system 8 in urea production is more than 99.5% enters in the urea solution tank 6 by the pipeline that flow meter 9 is installed;
[0035] Three, the sustained-release agent mixed in step 1 and the molten urea solution in step 2 are placed on the urea solution tank 6 and uniformly mixed, and the pressure of the urea solution tank 6 is 0.55MPa, and the temperature is 140°C;
[0036] 4. Put the mixed mixture in step 3 into the gran...
Embodiment 3
[0039] When making 3000 kg of the present invention, 360 kg of attapulgite powder, 30 kg of polyacrylamide, 30 kg of quartz stone powder and 2580 kg of molten urea solution.
[0040] 1. Put 360 kg of attapulgite powder, 30 kg of polyacrylamide, and 30 kg of quartz stone powder into the slow-release agent feeding device 1 and mix them into the urea solution tank 6 through the metering belt 2, the slow-release agent tank 4 and the powder pump 5 Inside;
[0041] Two, 2580 kilograms of molten urea solution that the concentration that comes from evaporation system 8 in urea production is more than 99.5% enters in the urea solution tank 6 by the pipeline that flow meter 9 is installed;
[0042] Three, the sustained-release agent mixed in the step 1 and the molten urea solution in the step 2 are placed on the urea solution tank 6 and uniformly mixed, and the pressure of the urea solution tank 6 is 0.6MPa, and the temperature is 145°C;
[0043] 4. Put the mixed mixture in step 3 into...