Embodiment 1
[0019] Lavender was used as a raw material, dried at 40° C. for 15 hours, pulverized with a rod mill, and then sieved with a 150-mesh sieve, and the granule powder with a 150-mesh sieve was selected for use. 25 g of ethyl cellulose used as a binder was injected into 1000 g of 95% ethanol solution and stirred at 30° C. for 2.5 hours to achieve complete dissolution.
[0020] Add 200g lavender powder into a mixer with a volume of 5L, then add 800g of the prepared binder solution and stir for 2 hours to achieve that the lavender powder is evenly dispersed in the binder solution. 40% is coated on the base paper of the cigarette paper filter material, and then embossed, dried, cut, and then shaped into a cigarette paper filter rod. According to the length ratio of 1:3, the composite filter rods of cigarette paper filter rods and ordinary cellulose acetate filter rods were prepared, and then rolled into paper filter rod cigarettes containing lavender powder.
Embodiment 2
[0022] The lavender was dried at 40° C. for 15 hours, pulverized with a rod mill, and then sieved with a 120-mesh sieve, and the granule powder of the 120-mesh sieve was selected for use. 55 g of methylcellulose used as a binder was injected into 1000 g of 95% ethanol solution, and it was stirred at 30° C. for 2.5 hours to achieve complete dissolution.
[0023] Adding the lavender powder with a weight of 300g into a mixer with a volume of 5L, adding 800g of the prepared binder solution and stirring for 2 hours to achieve that the lavender powder is evenly dispersed in the binder solution, the above-mentioned prepared lavender solution Coat 35% by weight on base paper of cigarette paper filter material, then emboss, dry, cut, and then shape into cigarette paper filter rod. According to the length ratio of 2:3, the composite filter rods of cigarette paper filter rods and common cellulose acetate filter rods were prepared, and then rolled into paper filter rod cigarettes containi...
Embodiment 3
[0025] The lavender was dried at 40° C. for 15 hours, pulverized with a rod mill, and then sieved with a 100-mesh sieve to select and use the 100-mesh sieve particle powder. 75 g of xylose used as a binder was injected into 1000 g of 95% ethanol solution, and it was stirred at 30° C. for 2.5 hours to achieve complete dissolution.
[0026] Adding the lavender powder with a weight of 400g into a mixer with a volume of 5L, then adding 800g of the prepared binder solution and stirring for 2 hours to achieve that the lavender powder is evenly dispersed in the binder solution, the above prepared lavender solution Coat 30% by weight on base paper of cigarette paper filter material, then emboss, dry, cut, and then shape into cigarette paper filter rod. According to the length ratio of 1:1, the composite filter rods of cigarette paper filter rods and ordinary cellulose acetate filter rods were prepared, and then rolled into paper filter rod cigarettes containing lavender powder.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com