Biodegradable agricultural water retaining material and preparation method thereof
A water-retaining material and biodegradable technology, applied in the field of composite materials, can solve the problems of affecting soil components, low production efficiency, etc., and achieve the effects of simple preparation method, high production efficiency and simple method
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0027] Add 25 parts of PBS, 30 parts of acrylic acid, 30 parts of cornstarch, 10 parts of glycerin, 5 parts of water and 0.3 parts of DCP into the mixer in sequence and mix them. After mixing evenly, release them for later use. Then put the mixture into the twin-screw extruder and extrude at 160°C. After the strands are naturally foamed, they are cooled by air cooling, then cut into pellets with a pelletizer, finally crushed, and sieved with 50 meshes to obtain light yellow Porous, water-retaining granules.
[0028] Each gram of pellets can absorb 423 grams of distilled water.
Embodiment 2
[0030] Mix 30 parts of PCL, 10 parts of sodium acrylate, 40 parts of wood powder, 15 parts of sorbitol, 5 parts of water, and 0.1 part of BIPB in a mixer in sequence, mix well and release for later use. Then put the mixture into the twin-screw extruder and extrude at 190°C. After the strands are naturally foamed, they are cooled by air cooling, then cut into pellets with a pelletizer, finally crushed, and sieved with 50 meshes to obtain light yellow Porous, water-retaining granules.
[0031] Each gram of pellets can absorb 572 grams of distilled water.
Embodiment 3
[0033] Mix 10 parts of PBAT (melting point 110-120oC), 20 parts of acrylamide, 50 parts of tapioca starch, 10 parts of polyethylene glycol (molecular weight 300), 10 parts of water, and 1 part of BPO in a mixer in sequence, mix well and release spare. Then put the mixture into the twin-screw extruder and extrude at 140°C. After the strands are naturally foamed, they are cooled by air cooling, then cut into pellets with a pelletizer, finally crushed, and sieved with 50 meshes to obtain light yellow Porous, water-retaining granules.
[0034] Each gram of pellets can absorb 586 grams of distilled water.
PUM
Property | Measurement | Unit |
---|---|---|
melting point | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com