A kind of inorganic glue plug and preparation method thereof
A technology of planting reinforcement bolts and planting reinforcement glues, applied in building maintenance, construction, building construction, etc., can solve the problems of cumbersome operation, high anchoring strength, and large steel holding force, and achieves simple operation and good anti-corrosion performance. , good applicability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0017] This implementation includes a solid glass tube plug and a liquid glass tube plug, and the mass ratio of the solid glass tube plug to the liquid glass tube plug is 1.8:1.
[0018] The solid glass tube plug is composed of a glass tube and S95 granulated blast furnace slag powder installed in the glass tube; the liquid glass tube plug is composed of a glass tube and a mixed solution of water glass and sodium hydroxide installed in the glass tube. The mass ratio to sodium hydroxide is 1:0.16.
[0019] The method for preparing the present embodiment comprises the following steps:
[0020] (1) Material preparation: Select two glass tubes with the same diameter and a wall thickness of 0.5mm according to the size of the planting bar hole, the depth of the planting bar and the material mix ratio;
[0021] (2) Preparation of solid glass tube glue plug: take a glass tube prepared in step (1), fill it with S95 granulated blast furnace slag powder, and then completely seal the gla...
Embodiment 2
[0028] This implementation includes a solid glass tube plug and a liquid glass tube plug, and the mass ratio of the solid glass tube plug to the liquid glass tube plug is 2.0:1.
[0029] The solid glass tube plug is composed of a glass tube and S95 granulated blast furnace slag powder and fly ash contained in the glass tube. The mass ratio of the S95 granulated blast furnace slag powder and fly ash is 1:0.2;
[0030] The liquid glass tube plug is composed of a glass tube and a mixed solution of water glass and sodium hydroxide in the glass tube, and the mass ratio of the water glass and sodium hydroxide is 1:0.1.
[0031] The method for preparing the present embodiment comprises the following steps:
[0032] (1) Material preparation: Select two glass tubes with the same diameter and a wall thickness of 0.5mm according to the size of the reinforcement hole, the depth of the reinforcement and the mix ratio;
[0033] (2) Preparation of solid glass tube glue plug: take a glass tu...
Embodiment 3
[0037] This implementation includes a solid glass tube plug and a liquid glass tube plug, and the mass ratio of the solid glass tube plug to the liquid glass tube plug is 2.2:1.
[0038] The solid glass tube plug is composed of a glass tube and S95 granulated blast furnace slag powder, fly ash and expansion agent contained in the glass tube. The mass ratio of the slag powder, fly ash and expansion agent is 100:10:5;
[0039] The liquid glass tube plug is composed of a glass tube and a mixed solution of water glass and sodium hydroxide in the glass tube, and the mass ratio of the water glass and sodium hydroxide is 1:0.18.
[0040] The method for preparing the present embodiment comprises the following steps:
[0041] (1) Material preparation: Select two glass tubes with the same diameter and a wall thickness of 0.5mm according to the size of the reinforcement hole, the depth of the reinforcement and the mix ratio;
[0042] (2) Preparation of solid glass tube glue plug: take a...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com