A synthesis method and technology of a combustion aid, applied in the field of new water-based coal-fired combustion aids and their synthesis, can solve the problem of low coal combustion rate and achieve the effects of improving combustion efficiency, improving combustion efficiency, and reducing environmental pollution
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0046] The technical solution adopted by the invention is a novel water-based coal-fired combustion-supporting agent, which is composed of potassium permanganate, potassium chlorate, borax, manganese dioxide, ferric oxide, suspending agent and water.
[0047] The steps of the synthetic method of this novel water-based coal-burning combustion-supporting agent are:
[0048] Preparation of suspending agent: add 675kg of water to the reactor at normal temperature, stir at a stirring speed of 120 rpm, then add 75kg of soluble cellulose to the reactor, and heat the reactants in the reactor to 80°C; Slowly add 200kg of sodium hydroxide aqueous solution into the reaction kettle at a rate of 20kg per minute, and the mass fraction of the sodium hydroxide aqueous solution is 30%. Add 50kg water glass, water glass is the sodium silicate aqueous solution that mass fraction is 10%, obtain described suspending agent after reacting at 80 ℃ for 0.5 hour.
[0049] Synthesis of a new type of wa...
Embodiment 2
[0051] Further, preferred implementations also include:
[0052] A novel water-based coal-burning combustion-supporting agent is composed of potassium permanganate, potassium chlorate, borax, manganese dioxide, ferric oxide, suspending agent and water.
[0053] The steps of the synthetic method of this novel water-based coal-burning combustion-supporting agent are:
[0054] Preparation of suspending agent: add 675kg of water to the reactor at normal temperature, stir at a stirring speed of 120 rpm, then add 75kg of soluble cellulose to the reactor, and heat the reactants in the reactor to 80°C; Slowly add 200kg of sodium hydroxide aqueous solution into the reaction kettle at a rate of 20kg per minute, and the mass fraction of the sodium hydroxide aqueous solution is 30%. Add 50kg water glass, water glass is the sodium silicate aqueous solution that mass fraction is 10%, obtain described suspending agent after reacting at 80 ℃ for 0.5 hour.
[0055] Synthesis of a new type of...
Embodiment 3
[0057] Further, preferred implementations also include:
[0058] A novel water-based coal-burning combustion-supporting agent is composed of potassium permanganate, potassium chlorate, borax, manganese dioxide, ferric oxide, suspending agent and water.
[0059] The steps of the synthetic method of this novel water-based coal-burning combustion-supporting agent are:
[0060] Preparation of suspending agent: add 675kg of water to the reactor at normal temperature, stir at a stirring speed of 120 rpm, then add 75kg of soluble cellulose to the reactor, and heat the reactants in the reactor to 80°C; Slowly add 200kg of sodium hydroxide aqueous solution into the reaction kettle at a rate of 20kg per minute, and the mass fraction of the sodium hydroxide aqueous solution is 30%. Add 50kg water glass, water glass is the sodium silicate aqueous solution that mass fraction is 10%, obtain described suspending agent after reacting at 80 ℃ for 0.5 hour.
[0061] Synthesis of a new type of...
PUM
Property | Measurement | Unit |
---|---|---|
quality score | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com