A method of spraying the surface of a mobile phone protective case
A mobile phone protective shell and coating technology, which is applied to the surface coating liquid device, pretreatment surface, coating, etc., can solve the problems of fading, rough style, and shorten the life of the internal parts of the mobile phone, etc., to achieve stable spray coating, long life effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0033] Embodiment one: a method for spraying the surface of a mobile phone protective case, comprising the following steps in turn:
[0034] Step 1: Eliminate static electricity on the surface of the product: Take the ion wind rod and move it back and forth at a uniform speed on the surface of the mobile phone protective case to remove static electricity. Charge, when the charge on the surface of the mobile phone protective case is negative, the positive charge in the airflow is absorbed by the ion wind rod, and when the charge on the surface of the mobile phone protective case is positive, the negative charge in the airflow is absorbed by the ion wind rod, In this way, the static electricity on the surface of the mobile phone protective case is neutralized to achieve the purpose of eliminating static electricity;
[0035] Step 2: Product preheating: place the mobile phone protective case in the heating furnace for preheating. The initial preheating temperature is 65-75°C. Whe...
Embodiment 2
[0057] The second embodiment is roughly the same as the first embodiment, except that the A component is composed of the following components and the mass percentage of each component is:
[0058]
[0059]
[0060] After readjusting the proportions of the components in the second embodiment, 65% hydroxy acrylic resin is used, which can save costs, but the heat dissipation effect and discoloration effect of the protective case of the mobile phone are still similar.
Embodiment 3
[0062] The third embodiment is roughly the same as the first embodiment, except that the A component is composed of the following components and the mass percentage of each component is:
[0063]
[0064] After the proportions of the components in Example 3 are re-adjusted, the use of 15% xylene can make the components more fully mixed with each other and make the coloring of the spray paint more stable.
PUM