A technology for textile fabrics, antibacterial and anti-inflammatory, applied in the processing of textile materials, textiles and papermaking, fiber processing, etc., can solve the problems of not being able to meet people's high quality of life, and achieve the effects of simple structure, low production cost, and reasonable settings
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0012] The technical scheme that present embodiment adopts is: its production process is as follows:
[0013] 1. After washing the wormwood with pure water, put it into distilled water and heat it to boiling. The mass ratio of wormwood to distilled water is 1:120 (the heating device is equipped with a reflux device, so that the steam generated by heating can be refluxed into the heating device), After heating for 40 minutes, cool, filter, remove the slag and take the liquid to obtain the soaking liquid;
[0014] Two, cotton fiber is put into above-mentioned soaking liquid and soaked, the mass ratio of cotton fiber and soaking liquid is 1:500, and soaking time is 10 days under room temperature;
[0015] 3. Take out the soaked cotton fibers, dry them naturally at room temperature, and put them into an oven for drying at a temperature of 50-150°C;
[0016] 4. Weaving the dried cotton fiber into cloth through textile process.
[0017] The beneficial effects of the present invent...
Embodiment 2
[0019] The technical scheme that present embodiment adopts is: its production process is as follows:
[0020] 1. After washing the wormwood with pure water, put it into distilled water and heat it to boiling. The mass ratio of wormwood to distilled water is 1:180 (the heating device is equipped with a reflux device to make the steam generated by heating return to the heating device), After heating for 50 minutes, cool, filter, remove the slag and take the liquid to obtain the soaking liquid;
[0021] 2. Soak the wool fiber in the above-mentioned soaking solution, the mass ratio of the textile fiber to the soaking solution is 1:800, and the soaking time at room temperature is 12 days;
[0022] 3. Take out the soaked wool fibers, dry them naturally at room temperature, and then put them into an oven for drying at a temperature of 50-130°C;
[0023] 4. Weaving the dried wool fiber into cloth through weaving process.
Embodiment 3
[0025] 1. After washing the wormwood with pure water, put it into distilled water and heat it to boiling. The mass ratio of wormwood to distilled water is 1:140 (the heating device is equipped with a reflux device, so that the steam generated by heating can be refluxed into the heating device), After heating for 40 minutes, cool, filter, remove the slag and take the liquid to obtain the soaking liquid;
[0026] Two, silk fiber is put into above-mentioned soaking liquid and soaked, and the mass ratio of silk fiber and soaking liquid is 1:200, and soaking time is 7 days under room temperature;
[0027] 3. Pull out the above-mentioned soaked silk fibers, dry them naturally at room temperature, and put them into an oven for drying at a temperature of 50-130°C;
[0028] 4. Weave the dried silk fiber into cloth through textile process.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com