An anti-micropitting and gear oil technology, applied in the petroleum industry, lubricating compositions, etc., can solve the problems that are difficult to perform long-term lubrication work and affect the performance of wind power gear oil, so as to improve the anti-micropitting performance and high Excellent shear stability and abrasion resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0046] The preparation method of the long-life anti-micropitting wind power gear oil of the present invention is as follows: add 1 / 2 synthetic base oil into the blending kettle, heat up to 85°C±5°C, add antioxidant V887E (0.1%) and RC7115 (0.2 %) and then stirred continuously for 1h. Add the remaining base oil, keep the temperature at 60°C and add the compounding agent (5.5%), continue stirring for 30 minutes, add molybdenum dialkyldithiocarbamate (0.3%), continue stirring for 30 minutes, and cool to obtain the finished product.
Embodiment 2
[0048] The preparation method of the long-life anti-micropitting wind power gear oil of the present invention is as follows: add 1 / 2 synthetic base oil into the blending kettle, heat up to 85°C±5°C, add antioxidants V887E (0.15%) and RC7115 (0.15%) %) and then stirred continuously for 1h. Add the remaining base oil, keep the temperature at 60°C and add the compounding agent (4%), continue stirring for 30 minutes, add molybdenum dialkyldithiocarbamate (0.5%), continue stirring for 30 minutes, and cool to obtain the finished product.
Embodiment 3
[0050] The preparation method of the long-life anti-micropitting wind power gear oil of the present invention is as follows: add 1 / 2 synthetic base oil into the blending kettle, heat up to 85°C±5°C, add antioxidant V887E (0.2%) and RC7115 (0.1 %) and then stirred continuously for 1h. Add the remaining base oil, keep the temperature at 60°C and add the compounding agent (3%), continue stirring for 30 minutes, add molybdenum dialkyldithiocarbamate (0.8%), continue stirring for 30 minutes, and cool to obtain the finished product.