Polyamino acid gel and preparation method and application thereof
A technology of polyamino acid gel and polyamino acid, applied in pharmaceutical formulations, cosmetic preparations, dressing preparations, etc., can solve the problems of non-compliance with new zero additives, narrow application fields, single dosage forms, etc., to increase skin elasticity , Improve the effect of mechanical strength and toughness
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0052] A preparation method of a polyamino acid gel, the preparation method comprising the following steps: putting the above components into a reactor with stirring function, adding a small amount of hydrochloric acid or sodium hydroxide to adjust the pH of the solution to 3-13, stirring for 15 ~60min, repeatedly adjust the pH of the solution, and let it stand at room temperature for 12~36h to complete the self-assembly of macromolecules and form a paste-like polyamino acid gel.
[0053] The application of the polyamino acid gel of the present invention in the preparation of facial mask or lotion, nutritional cream, essence, eye cream, hand cream, shampoo, hair conditioner and sunscreen.
[0054] Such as figure 1 As shown, the polyamino acid hydrogel facial mask of the present invention is a double network hydrogel made of the polyamino acid gel of the present invention, and the double network hydrogel includes at least one layer made of cyclodextrin The formed self-assemble...
Embodiment 1
[0060] A polyamino acid gel, calculated in parts by mass, its composition and consumption are as follows:
[0061]
[0062] The preparation method specifically comprises the following steps:
[0063] Weigh the above raw materials respectively and put them into the reaction equipment with stirring function, add a small amount of hydrochloric acid to adjust the pH to 6.5, stir for 30 minutes, and rotate at 100 rpm, then adjust the pH of the material liquid to 6.5, and let it stand at room temperature for 24 hours to form a transparent, uniform Liquid polyamino acid gel.
[0064] The obtained polyamino acid gel is added to the basic emulsion, which has a significant multiplied moisturizing effect on the active ingredients, which increases the overall moisturizing effect of the product by 45%, and improves the long-term moisturizing effect of the product.
Embodiment 2
[0066] A polyamino acid gel, calculated in parts by mass, its composition and consumption are as follows:
[0067]
[0068] The preparation method specifically comprises the following steps:
[0069] Weigh the above raw materials respectively and put them into the reaction equipment with stirring function, add a small amount of sodium hydroxide to adjust the pH to 8, stir for 40 minutes, and the rotation speed is 120rpm, then adjust the pH of the material liquid to 8, and let it stand at room temperature for 30 hours to obtain a transparent, viscous polyamino acid gel.
[0070] Adding the above-mentioned polyamino acid gel to the basic emulsion has a significant multiplied moisturizing effect on the active ingredients, which increases the overall moisturizing effect of the product by 45%, and improves the long-term moisturizing effect of the product to nourish the skin. Remove fine lines and solve the five major problems of light and mature skin.
PUM
Property | Measurement | Unit |
---|---|---|
molecular weight | aaaaa | aaaaa |
molecular weight | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com