Easy-defoaming violin paint and manufacturing method thereof
A technology of polymer and solid content, used in coatings, polyester coatings, etc., can solve problems such as poor defoaming of violin paint, and achieve the effect of preventing construction and ensuring rapidity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0010] Alkyd resin polymer (solid content 80%) 30 kg, styrene 15 kg, polyethylene glycol (600) 0.01 kg, dibutyltin dilaurate 1 kg, polyamide wax (n-butanol, naphtha mixture) 2 kg, 50 kg of o-phthalic unsaturated polyester resin, 10.1 kg of polyvinyl butyral, 10 kg of ethyl acetate, 0.1 kg of a hydrophobic solid mixture of defoaming polysiloxane and polyethylene glycol. Mix alkyd resin polymer (solid content 80%), styrene, polyethylene glycol (600), dibutyltin dilaurate and polyamide wax (n-butanol, naphtha mixture), and keep stirring for 30 minutes. Then add o-phthalic unsaturated polyester resin, polyvinyl butyral, ethyl acetate, defoaming polysiloxane and polyethylene glycol hydrophobic solid mixture, and continue to stir for 30 minutes.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More