A kind of amide compound, clay stabilizer, its preparation method and application
The technology of amide compound and clay stabilizer is applied in the field of amide compound, its preparation and clay stabilizer, which can solve the problems of increasing the cost of drilling fluid, adversely affecting the performance of drilling fluid, limiting the scope of application, etc. Stable product quality and controlling the effect of formation pulping
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0041] The invention provides a kind of preparation method of clay stabilizer, comprises the following steps:
[0042] The citric acid is reacted with polyethylene polyamine to obtain an amide compound; the polyethylene polyamine is selected from diethylene triamine, triethylene tetramine, tetraethylene pentamine, pentaethylene hexamine or hexaethylene heptamine; the Amide compounds have the structure of formula I:
[0043]
[0044] Wherein, n is selected from an integer between 1 and 5;
[0045] The material including the amide compound is discharged to obtain a clay stabilizer.
[0046] The invention synthesizes the clay stabilizer with amide groups and other groups through the amidation reaction, which has a good effect of inhibiting clay hydration and dispersion, and does not affect the performance of drilling fluid at the same time, which is beneficial to application.
[0047] In the present invention, citric acid and polyethylene polyamine are added into a reaction ...
Embodiment 1
[0061] Add citric acid and tetraethylenepentamine into the reaction flask with agitator and condensation according to the ratio of substances of 1:2.50, raise the temperature to 150°C, add 0.5% phenylboronic acid accounting for the mass of the reaction raw materials, and proceed at 170°C After amidation reaction for 2 hours, after the reaction time is up, cool down to 60°C, adjust the pH value to 6.5 with hydrochloric acid with a mass fraction of 18%, cool down to room temperature, and discharge the clay stabilizer for drilling fluid, which is a brown viscous liquid .
[0062] Inhibition rate evaluation method:
[0063] Take 350mL of distilled water, add 0.5% sodium carbonate, dissolve and add 10% calcium bentonite (calcium bentonite for drilling fluid produced by Weifang Huawei Bentonite Group Co., Ltd.), stir at high speed for 20 minutes, and roll at 120°C for 12 hours to obtain a blank Slurry: Take it out after cooling down, stir at high speed for 5 minutes, measure the vi...
Embodiment 2
[0068] Add citric acid and tetraethylenepentamine to the reaction bottle with agitator and condensation according to the ratio of substances of 1:3.05, raise the temperature to 150°C, add phenylboronic acid accounting for 2% of the mass of the reaction raw materials, and react at 150°C After 10 hours, after the reaction time is up, cool down to 60°C, adjust the pH value to 8.0 with 18% hydrochloric acid, cool down to room temperature, and discharge to obtain the clay stabilizer for drilling fluid, which is a brown viscous liquid.
[0069] The inhibition rate was evaluated according to the method in Example 1, and the results showed that the relative inhibition rate of the product was 91.8%.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com