Drizzle-crepe-appearance pure cotton yarn-dyed fabric production process
A production process and pure cotton technology, applied in the textile field, can solve the problems of large dimensional change rate and poor physical stability, and achieve the effects of elasticity, good physical stability, good skin-friendly and softness
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] 30-count cotton-dyed yarn-dyed fabric with wrinkled appearance. The technological process is: design of pattern and weave specifications→warp and weft yarn treatment→weaving→finishing.
[0022] In the design of weave specifications, the warp yarn is made of pure cotton combed yarn with a count of 30 pounds and the twist is 20T / in; Increase the twist to 16T / in, the weft arrangement is 1 S-twisted backward-twisted strong-twisted yarn and 1 Z-twisted backward-twisted strong-twisted yarn, the weave is plain weave, and the warp density is 70 yarns / inch. The weft density is 60 threads / inch.
[0023] The process flow of warp yarn treatment is as follows: loose winding → cheese bleaching → rewinding → warping → sizing → weaving, and the parameters of each process are the same as the conventional parameters.
[0024] The weft yarn treatment process is as follows: loose winding → bobbin bleaching → rewinding → secondary twisting → steamed yarn fixed twist → weaving. Among them,...
Embodiment 2
[0035] 40-count cotton-dyed yarn-dyed fabric with rain-shrink wrinkle appearance, the technological process is: design of pattern weave specification → warp and weft yarn treatment → weaving → finishing.
[0036] In the design of weave specifications, the warp yarn is made of pure cotton combed yarn of count 40, and the twist is 20T / in; Afterwards, the twist is increased to 20T / in, and the weft arrangement is 1 S-twisted backward-twisted strong-twisted yarn and 1 Z-twisted backward-twisted strong-twisted yarn, the weave is plain weave, and the warp density is 90 yarns / inch , weft density of 70 / inch.
[0037] The warp yarn treatment process is as follows: loose winding→cheese whitening→rewinding→warping→sizing→weaving, and the parameters of each process are the same as the conventional parameters.
[0038] The process flow of weft yarn treatment is as follows: loose winding → cheese whitening → rewinding → secondary twisting → steamed yarn fixed twist → weaving. Among them,...
Embodiment 3
[0049] 30-count cotton-dyed yarn-dyed fabric with delicate appearance of rain silk wrinkle. The technological process is: design of pattern weave specification→warp and weft yarn treatment→weaving→finishing.
[0050] In the design of weave specifications, the warp yarn is made of pure cotton combed yarn with a count of 30 pounds and the twist is 20T / in; Increase the twist to 18T / in, the weft arrangement is 1 S-twisted backward-twisted strong-twisted yarn and 1 Z-twisted backward-twisted strong-twisted yarn, the weave is plain weave, and the warp density is 80 yarns / inch. The weft density is 70 threads / inch.
[0051] The process flow of warp yarn treatment is as follows: loose winding → cheese bleaching → rewinding → warping → sizing → weaving, and the parameters of each process are the same as the conventional parameters.
[0052] The weft yarn treatment process is as follows: loose winding → bobbin bleaching → rewinding → secondary twisting → steamed yarn fixed twist → weavi...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology