Nano leather nourishing essence lotion and preparation method thereof
A technology of essence milk and leather, applied in the field of daily necessities, to achieve the effect of excellent water resistance, wet rub resistance and abrasion resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0027] Embodiment 1 A kind of nano-leather nourishing essence milk
[0028] Composition of raw materials by weight: 20% silicone, 8% lanolin, 20% Brazilian wax, 3% emulsifier,
[0029] Essence 3%, leather antifungal agent 3%, and the balance is water.
[0030] The organosilicon is a modified organosilicon, and the modified organosilicon is prepared by the following method:
[0031] (1) Dissolve rosin resin in an organic solvent, then add silicone resin, coupling agent and catalyst to obtain a reaction solution; (2) Put the reaction solution in a reaction kettle for 2 hours at 135 degrees Celsius, and decompress Concentrate, remove the organic solvent, and obtain the modified silicone after drying; the weight ratio of the silicone resin, rosin resin, coupling agent and catalyst is 100:25:1:1; the The coupling agent is silane coupling agent kh550; the catalyst is benzoyl peroxide.
[0032] The preparation method of nano leather nourishing essence milk:
[0033] (1) Heat to m...
Embodiment 2
[0038] Embodiment 2 A kind of nano-leather nourishing essence milk
[0039] Composition of raw materials by weight: 15% silicone, 10% lanolin, 10% Brazilian wax, 3% emulsifier,
[0040] Essence 3%, leather antifungal agent 3%, and the balance is water.
[0041] The organosilicon is a modified organosilicon, and the modified organosilicon is prepared by the following method:
[0042] (1) Dissolve rosin resin in an organic solvent, then add silicone resin, coupling agent and catalyst to obtain a reaction solution; (2) Put the reaction solution in a reaction kettle for 3 hours at 120 degrees Celsius, and then reduce pressure Concentrate, remove the organic solvent, and obtain the modified silicone after drying; the weight ratio of the silicone resin, rosin resin, coupling agent and catalyst is 100:20:2:2; the The coupling agent is silane coupling agent kh550; the catalyst is benzoyl peroxide.
[0043] The preparation method of nano leather nourishing essence milk:
[0044] (1...
Embodiment 3
[0049] Embodiment 3 A kind of nano-leather nourishing essence milk
[0050] Composition of raw materials by weight: 30% silicone, 5% lanolin, 20% Brazilian wax, 3% emulsifier,
[0051] Essence 3%, leather antifungal agent 3%, and the balance is water.
[0052] The organosilicon is a modified organosilicon, and the modified organosilicon is prepared by the following method:
[0053] (1) Dissolve rosin resin in an organic solvent, then add silicone resin, coupling agent and catalyst to obtain a reaction solution; (2) Put the reaction solution in a reaction kettle for 3 hours at 120 degrees Celsius, and then reduce pressure Concentrate, remove the organic solvent, and obtain the modified silicone after drying; the weight ratio of the silicone resin, rosin resin, coupling agent and catalyst is 100:20:2:2; the The coupling agent is silane coupling agent kh550; the catalyst is benzoyl peroxide.
[0054] The preparation method of nano leather nourishing essence milk:
[0055] (1)...