[0033] A preparation method for preparing environmentally friendly art paint, said method comprising the steps of:
[0034] (1) Grind hexacyclite into powder particles with a particle size of no more than 30 μm, then soak in deionized water for 30 minutes to completely infiltrate, and the bamboo charcoal fiber is broken so that the length does not exceed 3 cm;
[0035] (2) Nano-silica modified acrylic resin emulsion, impregnated hexacyclite, HY-1608A, anionic dispersant, SILRES BS198, polyether polyester modified organosiloxane, BYK-024 and the remaining Slowly add ionized water into the stirring tank one by one, and stir for 30 to 40 minutes at a speed of 800 to 1000 r / min;
[0036] (3) Add Texanol and hydroxyethyl cellulose in sequence, and stir for 30-40 minutes at a speed of 800-1000 r / min;
[0037] (4) Add bamboo charcoal fiber and stir for 20-30 minutes at a speed of 1000-1200r / min to obtain the required environmental protection art paint.
[0038] In terms of parts by...
Embodiment 2
[0040] A preparation method for preparing environmentally friendly art paint, said method comprising the steps of:
[0041] (1) Grind hexacyclite into powder particles with a particle size of no more than 30 μm, then soak in deionized water for 30 minutes to completely infiltrate, and the bamboo charcoal fiber is broken so that the length does not exceed 3 cm;
[0042] (2) Nano-silica modified acrylic resin emulsion, impregnated hexacyclite, HY-1608A, anionic dispersant, SILRES BS198, polyether polyester modified organosiloxane, BYK-024 and the remaining Slowly add ionized water into the stirring tank one by one, and stir for 30 to 40 minutes at a speed of 800 to 1000 r / min;
[0043] (3) Add Texanol and hydroxyethyl cellulose in sequence, and stir for 30-40 minutes at a speed of 800-1000 r / min;
[0044] (4) Add bamboo charcoal fiber and stir for 20-30 minutes at a speed of 1000-1200r / min to obtain the required environmental protection art paint.
[0045]In terms of parts by ...
Embodiment 3
[0047] A preparation method for preparing environmentally friendly art paint, said method comprising the steps of:
[0048] (1) Grind hexacyclite into powder particles with a particle size of no more than 30 μm, then soak in deionized water for 30 minutes to completely infiltrate, and the bamboo charcoal fiber is broken so that the length does not exceed 3 cm;
[0049] (2) Nano-silica modified acrylic resin emulsion, impregnated hexacyclite, HY-1608A, anionic dispersant, SILRES BS198, polyether polyester modified organosiloxane, BYK-024 and the remaining Slowly add ionized water into the stirring tank one by one, and stir for 30 to 40 minutes at a speed of 800 to 1000 r / min;
[0050] (3) Add Texanol and hydroxyethyl cellulose in sequence, and stir for 30-40 minutes at a speed of 800-1000 r / min;
[0051] (4) Add bamboo charcoal fiber and stir for 20-30 minutes at a speed of 1000-1200r / min to obtain the required environmental protection art paint.
[0052] In terms of parts by...