Manufacturing method of wood for outdoor garden
A production method and wood technology are applied in the production field of wood for outdoor gardens, which can solve the problems of mold generation, waste of manpower and material resources, cracking, etc., and achieve the effects of prolonging service life, fast washing speed and simple process.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] A method for making wood for outdoor gardens, the method comprising the following steps:
[0022] S1. Drying: Select the sapwood of the wood, cut and process the selected wood according to the required specifications, and then dry it continuously for 4.5 days at 80°C to obtain a dry wood piece with a moisture content of 12%. The sapwood is hard and has scars. Small knots are easy to soak, more suitable for outdoor garden wood;
[0023] S2. Vacuum degreasing: place the dry wood piece in a closed degreasing tank, reduce the air pressure in the degreasing tank to vacuum condition, and keep it for 1 hour to obtain the degreasing wood piece;
[0024] S3. Inject flame retardant: inject liquid wax flame retardant setting agent into the degreased wood piece, and slowly heat up to 120°C;
[0025] S4. Pressurized wax replenishment: under continuous pressure of 150Kpa, continue to replenish phase and inject liquid wax flame retardant setting agent, and continue to treat for 8 hou...
Embodiment 2
[0029] A method for making wood for outdoor gardens, the method comprising the following steps:
[0030] S1. Drying: Select the sapwood of the wood, cut and process the selected wood according to the required specifications, and then dry it continuously for 5 days at 70°C to obtain a dry wood piece with a moisture content of 10%. The sapwood is hard and scars Small knots are easy to soak, more suitable for outdoor garden wood;
[0031] S2. Vacuum degreasing: place the dry wood piece in a closed degreasing tank, reduce the air pressure in the degreasing tank to vacuum condition, and keep it for 1 hour to obtain the degreasing wood piece;
[0032] S3. Inject flame retardant: inject liquid wax flame retardant setting agent into the degreased wood piece, and slowly heat up to 120°C;
[0033] S4. Pressurized wax replenishment: under continuous pressure of 150Kpa, continue to replenish phase and inject liquid wax flame retardant setting agent, and continue to treat for 7 hours;
...
Embodiment 3
[0037] A method for making wood for outdoor gardens, the method comprising the following steps:
[0038] S1. Drying: Select the sapwood of the wood, cut and process the selected wood according to the required specifications, and then dry it continuously for 5 days at 75°C to obtain a dry wood piece with a moisture content of 11%. The sapwood is hard and has scars. Small knots are easy to soak, more suitable for outdoor garden wood;
[0039] S2. Vacuum degreasing: place the dry wood piece in a closed degreasing tank, reduce the air pressure in the degreasing tank to vacuum condition, and keep it for 1 hour to obtain the degreasing wood piece;
[0040] S3. Inject flame retardant: inject liquid wax flame retardant setting agent into the degreased wood piece, and slowly heat up to 120°C;
[0041] S4. Pressurized wax replenishment: under continuous pressure of 160Kpa, continue to replenish phase and inject liquid wax flame retardant setting agent, and continue to treat for 8 hours...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com