no. 1 approach
[0055] In this embodiment, the first cutting groove 1 is formed by cutting the battery sheet on the first slicing line A, including:
[0056]The battery sheet is cut along the first slicing line A by using a laser, and the first cutting groove 1 with a first preset depth extending from one end to the other end is formed on the battery sheet.
[0057] The second cutting groove 2 is formed by cutting the battery sheet on the second slicing line B, including;
[0058] Use a laser to cut the battery sheet along the second slicing line B at intervals to form at least two of the second cutting grooves 2 arranged at intervals;
[0059] The battery sheet is further split along the first cutting groove 1 and the second cutting groove 2 to form four sub-sections, including:
[0060] The battery sheet is heated along the second slicing line B by a laser, and the battery sheet is split along the second cutting groove 2 to form two slicing;
[0061] The battery sheet is broken off along ...
no. 2 approach
[0068] In this embodiment, the first cutting groove 1 is formed by cutting the battery sheet on the first slicing line A, including:
[0069] The battery sheet is cut along the first slicing line A by using a laser, and the first cutting groove 1 with a first preset depth extending from one end to the other end is formed on the battery sheet.
[0070] The second cutting groove 2 is formed by cutting the battery sheet on the second slicing line B, including;
[0071] The battery sheet is cut along the second slicing line B by a laser, and a second cutting groove 2 with a second preset depth extending from one end to the other end is formed on the battery sheet. The depth is less than the first preset depth. That is, the depth of the first cutting groove 1 is set to be able to easily break the battery sheet, and the depth of the second cutting groove 2 is set to be able to be further split along the second cutting groove 2 when the battery sheet is heated.
[0072] The battery...
no. 3 approach
[0080] In this embodiment, the first cutting groove 1 is formed by cutting the battery sheet on the first slicing line A, including:
[0081] A laser is used to cut the battery sheet along the first slicing line A at intervals to form at least two of the first cutting grooves 1 arranged at intervals.
[0082] The second cutting groove 2 is formed by cutting the battery sheet on the second slicing line B, including;
[0083] Use a laser to cut the battery sheet along the second slicing line B at intervals to form at least two of the second cutting grooves 2 arranged at intervals;
[0084] The battery sheet is further split along the first cutting groove 1 and the second cutting groove 2 to form four sub-sections, including:
[0085] The battery sheet is heated along the first slicing line A and the second slicing line B by a laser, and the battery sheet is split along the first cutting groove 1 and the second cutting groove 2 to form Four shards.
[0086] Wherein, in this em...